Carbon nanotubes (CNTs) are allotropes of carbon with a cylindrical nanostructure. Nanotubes have been constructed with length-to-diameter ratio of up to 132,000,000:1,[1] significantly larger than for any other material. These cylindrical carbon molecules have unusual properties, which are valuable for nanotechnology, electronics, optics and other fields of materials science and technology. In particular, owing to their extraordinary thermal conductivity and mechanical and electrical properties, carbon nanotubes may find applications as additives to various structural materials.
Nanotubes are members of the fullerene structural family, which also includes the spherical buckyballs, and the ends of a nanotube may be capped with a hemisphere of the buckyball structure. Their name is derived from their long, hollow structure with the walls formed by one-atom-thick sheets of carbon, called graphene. These sheets are rolled at specific and discrete ("chiral") angles, and the combination of the rolling angle and radius decides the nanotube properties; for example, whether the individual nanotube shell is a metal or semiconductor. Nanotubes are categorized as single-walled nanotubes (SWNTs) and multi-walled nanotubes (MWNTs). Individual nanotubes naturally align themselves into "ropes" held together by van der Waals forces.
Applied quantum chemistry, specifically, orbital hybridization best describes chemical bonding in nanotubes. The chemical bonding of nanotubes is composed entirely of sp2 bonds, similar to those of graphite. These bonds, which are stronger than the sp3 bonds found in alkanes, provide nanotubules with their unique strength.

 

Types of carbon nanotubes and related structures

Terminology

There is no consensus on some terms describing carbon nanotubes in scientific literature: both "-wall" and "-walled" are being used in combination with "single", "double", "triple" or "multi", and the letter C is often omitted in the abbreviation; for example, multi-walled carbon nanotube (MWNT).

Single-walled


The (n,m) nanotube naming scheme can be thought of as a vector (Ch) in an infinite graphene sheet that describes how to "roll up" the graphene sheet to make the nanotube. T denotes the tube axis, and a1 and a2 are the unit vectors of graphene in real space.

A scanning tunneling microscopy image of single-walled carbon nanotube

A transmission electron microscopy image of a single-walled carbon nanotube
Most single-walled nanotubes (SWNT) have a diameter of close to 1 nanometer, with a tube length that can be many millions of times longer. The structure of a SWNT can be conceptualized by wrapping a one-atom-thick layer of graphite called graphene into a seamless cylinder. The way the graphene sheet is wrapped is represented by a pair of indices (n,m) . The integers n and m denote the number of unit vectors along two directions in the honeycomb crystal lattice of graphene. If m = 0, the nanotubes are called zigzag nanotubes, and if n = m, the nanotubes are called armchair nanotubes. Otherwise, they are called chiral. The diameter of an ideal nanotube can be calculated from its (n,m) indices as follows
 d = \frac{a}{\pi} \sqrt{(n^2 + nm + m^2)}.
where a = 0.246 nm.
SWNTs are an important variety of carbon nanotube because most of their properties change significantly with the (n,m) values, and this dependence is non-monotonic (see Kataura plot). In particular, their band gap can vary from zero to about 2 eV and their electrical conductivity can show metallic or semiconducting behavior. One useful application of SWNTs is in the development of the first intramolecular field-effect transistors (FET). Production of the first intramolecular logic gate using SWNT FETs has recently become possible as well.[2] To create a logic gate you must have both a p-FET and an n-FET. Because SWNTs are p-FETs when exposed to oxygen and n-FETs otherwise, it is possible to protect half of an SWNT from oxygen exposure, while exposing the other half to oxygen. This results in a single SWNT that acts as a NOT logic gate with both p and n-type FETs within the same molecule.
Single-walled nanotubes are dropping precipitously in price, from around $1500 per gram as of 2000 to retail prices of around $50 per gram of as-produced 40–60% by weight SWNTs as of March 2010.[3][4]

Multi-walled


A scanning electron microscopy image of carbon nanotubes bundles

Triple-walled armchair carbon nanotube
Multi-walled nanotubes (MWNT) consist of multiple rolled layers (concentric tubes) of graphite. There are two models that can be used to describe the structures of multi-walled nanotubes. In the Russian Doll model, sheets of graphite are arranged in concentric cylinders, e.g., a (0,8) single-walled nanotube (SWNT) within a larger (0,17) single-walled nanotube. In the Parchment model, a single sheet of graphite is rolled in around itself, resembling a scroll of parchment or a rolled newspaper. The interlayer distance in multi-walled nanotubes is close to the distance between graphene layers in graphite, approximately 3.4 Å. The Russian Doll structure is observed more commonly. Its individual shells can be described as SWNTs, which can be metallic or semiconducting. Because of statistical probability and restrictions on the relative diameters of the individual tubes, one of the shells, and thus the whole MWNT, is usually a zero-gap metal.
Double-walled carbon nanotubes (DWNT) form a special class of nanotubes because their morphology and properties are similar to those of SWNT but their resistance to chemicals is significantly improved. This is especially important when functionalization is required (this means grafting of chemical functions at the surface of the nanotubes) to add new properties to the CNT. In the case of SWNT, covalent functionalization will break some C=C double bonds, leaving "holes" in the structure on the nanotube and, thus, modifying both its mechanical and electrical properties. In the case of DWNT, only the outer wall is modified. DWNT synthesis on the gram-scale was first proposed in 2003[5] by the CCVD technique, from the selective reduction of oxide solutions in methane and hydrogen.
The telescopic motion ability of inner shells [6] and their unique mechanical properties [7] permit to use multi-walled nanotubes as main movable arms in coming nanomechanical devices. Retraction force that occurs to telescopic motion caused by the Lennard-Johnes interaction between shells and it's value is about 1.5 nN.[8]

Torus


A stable nanobud structure
In theory, a nanotorus is a carbon nanotube bent into a torus (doughnut shape). Nanotori are predicted to have many unique properties, such as magnetic moments 1000 times larger than previously expected for certain specific radii.[9] Properties such as magnetic moment, thermal stability, etc. vary widely depending on radius of the torus and radius of the tube.[9][10]

Nanobud

Carbon nanobuds are a newly created material combining two previously discovered allotropes of carbon: carbon nanotubes and fullerenes. In this new material, fullerene-like "buds" are covalently bonded to the outer sidewalls of the underlying carbon nanotube. This hybrid material has useful properties of both fullerenes and carbon nanotubes. In particular, they have been found to be exceptionally good field emitters. In composite materials, the attached fullerene molecules may function as molecular anchors preventing slipping of the nanotubes, thus improving the composite’s mechanical properties.

Cup stacked carbon nanotubes

Cup-stacked carbon nanotubes (CSCNTs) differ from other quasi-1D carbon structures, which normally behave as quasi-metallic conductors of electrons. CSCNTs exhibit semiconducting behaviors due to the stacking microstructure of graphene layers.[11]

Extreme carbon nanotubes


Cycloparaphenylene
The observation of the longest carbon nanotubes (18.5 cm long) was reported in 2009. These nanotubes were grown on Si substrates using an improved chemical vapor deposition (CVD) method and represent electrically uniform arrays of single-walled carbon nanotubes.[1]
The shortest carbon nanotube is the organic compound cycloparaphenylene, which was synthesized in early 2009.[12][13][14]
The thinnest carbon nanotube is armchair (2,2) CNT with a diameter of 3 Å. This nanotube was grown inside a multi-walled carbon nanotube. Assigning of carbon nanotube type was done by combination of high-resolution transmission electron microscopy (HRTEM), Raman spectroscopy and density functional theory (DFT) calculations.[15]
The thinnest freestanding single-walled carbon nanotube is about 4.3 Å in diameter. Researchers suggested that it can be either (5,1) or (4,2) SWCNT, but exact type of carbon nanotube remains questionable.[16] (3,3), (4,3) and (5,1) carbon nanotubes (all about 4 Å in diameter) were unambiguously identified using more precise aberration-corrected high-resolution transmission electron microscopy. However, they were found inside of double-walled carbon nanotubes.[17]

Properties

Strength

Carbon nanotubes are the strongest and stiffest materials yet discovered in terms of tensile strength and elastic modulus respectively. This strength results from the covalent sp2 bonds formed between the individual carbon atoms. In 2000, a multi-walled carbon nanotube was tested to have a tensile strength of 63 gigapascals (GPa).[18] (For illustration, this translates into the ability to endure tension of a weight equivalent to 6422 kg on a cable with cross-section of 1 mm2.) Further studies, conducted in 2008, revealed that individual CNT shells have strengths of up to ~100 GPa, which is in good agreement with quantum/atomistic models.[19] Since carbon nanotubes have a low density for a solid of 1.3 to 1.4 g/cm3,[20] its specific strength of up to 48,000 kN·m·kg−1 is the best of known materials, compared to high-carbon steel's 154 kN·m·kg−1.
Under excessive tensile strain, the tubes will undergo plastic deformation, which means the deformation is permanent. This deformation begins at strains of approximately 5% and can increase the maximum strain the tubes undergo before fracture by releasing strain energy.
Although the strength of individual CNT shells is extremely high, weak shear interactions between adjacent shells and tubes leads to significant reductions in the effective strength of multi-walled carbon nanotubes and carbon nanotube bundles down to only a few GPa’s.[21] This limitation has been recently addressed by applying high-energy electron irradiation, which crosslinks inner shells and tubes, and effectively increases the strength of these materials to ~60 GPa for multi-walled carbon nanotubes[19] and ~17 GPa for double-walled carbon nanotube bundles.[21]
CNTs are not nearly as strong under compression. Because of their hollow structure and high aspect ratio, they tend to undergo buckling when placed under compressive, torsional, or bending stress.[22]
Comparison of mechanical properties[23][24][25][26]
Material Young's modulus (TPa) Tensile strength (GPa) Elongation at break (%)
SWNTE ~1 (from 1 to 5) 13–53 16
Armchair SWNTT 0.94 126.2 23.1
Zigzag SWNTT 0.94 94.5 15.6–17.5
Chiral SWNT 0.92

MWNTE 0.2[18]–0.8[27]–0.95[18] 11[18]–63[18]–150[27]
Stainless steelE 0.186[28]–0.214[29] 0.38[28]–1.55[29] 15–50
Kevlar–29&149E 0.06–0.18[30] 3.6–3.8[30] ~2
EExperimental observation; TTheoretical prediction

The above discussion referred to axial properties of the nanotube, whereas simple geometrical
 considerations suggest that carbon nanotubes should be much softer in the radial direction than along the tube axis. Indeed, TEM observation of radial elasticity suggested that even the van der Waals forces can deform two adjacent nanotubes.[31] Nanoindentation experiments, performed by several groups on multiwalled carbon nanotubes [32][33] and tapping/contact mode atomic force microscope measurement performed on single-walled carbon nanotube,[34] indicated Young's modulus of the order of several GPa confirming that CNTs are indeed rather soft in the radial direction.

Hardness

Standard single-walled carbon nanotubes can withstand a pressure up to 24GPa without deformation. They then undergo a transformation to superhard phase nanotubes. Maximum pressures measured using current experimental techniques are around 55GPa. However, these new superhard phase nanotubes collapse at an even higher, albeit unknown, pressure.
The bulk modulus of superhard phase nanotubes is 462 to 546 GPa, even higher than that of diamond(420 GPa for single diamond crystal). [35]

Kinetic

Multi-walled nanotubes are multiple concentric nanotubes precisely nested within one another. These exhibit a striking telescoping property whereby an inner nanotube core may slide, almost without friction, within its outer nanotube shell, thus creating an atomically perfect linear or rotational bearing. This is one of the first true examples of molecular nanotechnology, the precise positioning of atoms to create useful machines. Already, this property has been utilized to create the world's smallest rotational motor.[36] Future applications such as a gigahertz mechanical oscillator are also envisaged.

Electrical


Band structures computed using tight binding approximation for (6,0) CNT (zigzag, metallic) (10,2) CNT (semiconducting) and (10,10) CNT (armchair, metallic).
Because of the symmetry and unique electronic structure of graphene, the structure of a nanotube strongly affects its electrical properties. For a given (n,m) nanotube, if n = m, the nanotube is metallic; if n − m is a multiple of 3, then the nanotube is semiconducting with a very small band gap, otherwise the nanotube is a moderate semiconductor. Thus all armchair (n = m) nanotubes are metallic, and nanotubes (6,4), (9,1), etc. are semiconducting.[37]
However, this rule has exceptions, because curvature effects in small diameter carbon nanotubes can strongly influence electrical properties. Thus, a (5,0) SWCNT that should be semiconducting in fact is metallic according to the calculations. Likewise, vice versa-- zigzag and chiral SWCNTs with small diameters that should be metallic have finite gap (armchair nanotubes remain metallic).[37] In theory, metallic nanotubes can carry an electric current density of 4 × 109 A/cm2, which is more than 1,000 times greater than those of metals such as copper,[38] where for copper interconnects current densities are limited by electromigration.
Multiwalled carbon nanotubes with interconnected inner shells show superconductivity with a relatively high transition temperature Tc = 12 K. In contrast, the Tc value is an order of magnitude lower for ropes of single-walled carbon nanotubes or for MWNTs with usual, non-interconnected shells.[39]

Optical

Thermal

All nanotubes are expected to be very good thermal conductors along the tube, exhibiting a property known as "ballistic conduction", but good insulators laterally to the tube axis. Measurements show that a SWNT has a room-temperature thermal conductivity along its axis of about 3500 W·m−1·K−1;[40] compare this to copper, a metal well known for its good thermal conductivity, which transmits 385 W·m−1·K−1. A SWNT has a room-temperature thermal conductivity across its axis (in the radial direction) of about 1.52 W·m−1·K−1,[41] which is about as thermally conductive as soil. The temperature stability of carbon nanotubes is estimated to be up to 2800 °C in vacuum and about 750 °C in air.[42]

Defects

As with any material, the existence of a crystallographic defect affects the material properties. Defects can occur in the form of atomic vacancies. High levels of such defects can lower the tensile strength by up to 85%. Another form of carbon nanotube defect is the Stone Wales defect, which creates a pentagon and heptagon pair by rearrangement of the bonds. Because of the very small structure of CNTs, the tensile strength of the tube is dependent on its weakest segment in a similar manner to a chain, where the strength of the weakest link becomes the maximum strength of the chain.
Crystallographic defects also affect the tube's electrical properties. A common result is lowered conductivity through the defective region of the tube. A defect in armchair-type tubes (which can conduct electricity) can cause the surrounding region to become semiconducting, and single monoatomic vacancies induce magnetic properties.[43]
Crystallographic defects strongly affect the tube's thermal properties. Such defects lead to phonon scattering, which in turn increases the relaxation rate of the phonons. This reduces the mean free path and reduces the thermal conductivity of nanotube structures. Phonon transport simulations indicate that substitutional defects such as nitrogen or boron will primarily lead to scattering of high-frequency optical phonons. However, larger-scale defects such as Stone Wales defects cause phonon scattering over a wide range of frequencies, leading to a greater reduction in thermal conductivity.[44]

One-dimensional transport

Because of the nanoscale dimensions, electrons propagate only along the tube's axis and electron transport involves many quantum effects. Because of this, carbon nanotubes are frequently referred to as “one-dimensional”.

Toxicity

The toxicity of carbon nanotubes has been an important question in nanotechnology. Such research has just begun. The data are still fragmentary and subject to criticism. Preliminary results highlight the difficulties in evaluating the toxicity of this heterogeneous material. Parameters such as structure, size distribution, surface area, surface chemistry, surface charge, and agglomeration state as well as purity of the samples, have considerable impact on the reactivity of carbon nanotubes. However, available data clearly show that, under some conditions, nanotubes can cross membrane barriers, which suggests that, if raw materials reach the organs, they can induce harmful effects such as inflammatory and fibrotic reactions.[45]
A study led by Alexandra Porter from the University of Cambridge shows that CNTs can enter human cells and accumulate in the cytoplasm, causing cell death.[46]
Results of rodent studies collectively show that regardless of the process by which CNTs were synthesized and the types and amounts of metals they contained, CNTs were capable of producing inflammation, epithelioid granulomas (microscopic nodules), fibrosis, and biochemical/toxicological changes in the lungs.[47] Comparative toxicity studies in which mice were given equal weights of test materials showed that SWCNTs were more toxic than quartz, which is considered a serious occupational health hazard when chronically inhaled. As a control, ultrafine carbon black was shown to produce minimal lung responses.[48]
The needle-like fiber shape of CNTs is similar to asbestos fibers. This raises the idea that widespread use of carbon nanotubes may lead to pleural mesothelioma, a cancer of the lining of the lungs or peritoneal mesothelioma, a cancer of the lining of the abdomen (both caused by exposure to asbestos). A recently-published pilot study supports this prediction.[49] Scientists exposed the mesothelial lining of the body cavity of mice to long multiwalled carbon nanotubes and observed asbestos-like, length-dependent, pathogenic behavior that included inflammation and formation of lesions known as granulomas. Authors of the study conclude:
"This is of considerable importance, because research and business communities continue to invest heavily in carbon nanotubes for a wide range of products under the assumption that they are no more hazardous than graphite. Our results suggest the need for further research and great caution before introducing such products into the market if long-term harm is to be avoided."[49]
According to co-author Dr. Andrew Maynard:
"This study is exactly the kind of strategic, highly focused research needed to ensure the safe and responsible development of nanotechnology. It looks at a specific nanoscale material expected to have widespread commercial applications and asks specific questions about a specific health hazard. Even though scientists have been raising concerns about the safety of long, thin carbon nanotubes for over a decade, none of the research needs in the current U.S. federal nanotechnology environment, health and safety risk research strategy address this question."[50]
Although further research is required, the available data suggests that under certain conditions, especially those involving chronic exposure, carbon nanotubes can pose a serious risk to human health.[45][46][48][49]

Synthesis


Powder of carbon nanotubes
Techniques have been developed to produce nanotubes in sizeable quantities, including arc discharge, laser ablation, high pressure carbon monoxide (HiPco), and chemical vapor deposition (CVD). Most of these processes take place in vacuum or with process gases. CVD growth of CNTs can occur in vacuum or at atmospheric pressure. Large quantities of nanotubes can be synthesized by these methods; advances in catalysis and continuous growth processes are making CNTs more commercially viable.

Arc discharge

Nanotubes were observed in 1991 in the carbon soot of graphite electrodes during an arc discharge, by using a current of 100 amps, that was intended to produce fullerenes.[51] However the first macroscopic production of carbon nanotubes was made in 1992 by two researchers at NEC's Fundamental Research Laboratory.[52] The method used was the same as in 1991. During this process, the carbon contained in the negative electrode sublimates because of the high discharge temperatures. Because nanotubes were initially discovered using this technique, it has been the most widely-used method of nanotube synthesis.
The yield for this method is up to 30% by weight and it produces both single- and multi-walled nanotubes with lengths of up to 50 micrometers with few structural defects.[20]

Laser ablation

In the laser ablation process, a pulsed laser vaporizes a graphite target in a high-temperature reactor while an inert gas is bled into the chamber. Nanotubes develop on the cooler surfaces of the reactor as the vaporized carbon condenses. A water-cooled surface may be included in the system to collect the nanotubes.
This process was developed by Dr. Richard Smalley and co-workers at Rice University, who at the time of the discovery of carbon nanotubes, were blasting metals with a laser to produce various metal molecules. When they heard of the existence of nanotubes they replaced the metals with graphite to create multi-walled carbon nanotubes.[53] Later that year the team used a composite of graphite and metal catalyst particles (the best yield was from a cobalt and nickel mixture) to synthesize single-walled carbon nanotubes.[54]
The laser ablation method yields around 70% and produces primarily single-walled carbon nanotubes with a controllable diameter determined by the reaction temperature. However, it is more expensive than either arc discharge or chemical vapor deposition.[20]

Chemical vapor deposition (CVD)


Nanotubes being grown by plasma enhanced chemical vapor deposition
The catalytic vapor phase deposition of carbon was first reported in 1959,[55] but it was not until 1993[56] that carbon nanotubes were formed by this process. In 2007, researchers at the University of Cincinnati (UC) developed a process to grow aligned carbon nanotube arrays of 18 mm length on a FirstNano ET3000 carbon nanotube growth system.[57]
During CVD, a substrate is prepared with a layer of metal catalyst particles, most commonly nickel, cobalt,[58] iron, or a combination.[59] The metal nanoparticles can also be produced by other ways, including reduction of oxides or oxides solid solutions. The diameters of the nanotubes that are to be grown are related to the size of the metal particles. This can be controlled by patterned (or masked) deposition of the metal, annealing, or by plasma etching of a metal layer. The substrate is heated to approximately 700°C. To initiate the growth of nanotubes, two gases are bled into the reactor: a process gas (such as ammonia, nitrogen or hydrogen) and a carbon-containing gas (such as acetylene, ethylene, ethanol or methane). Nanotubes grow at the sites of the metal catalyst; the carbon-containing gas is broken apart at the surface of the catalyst particle, and the carbon is transported to the edges of the particle, where it forms the nanotubes. This mechanism is still being studied. The catalyst particles can stay at the tips of the growing nanotube during the growth process, or remain at the nanotube base, depending on the adhesion between the catalyst particle and the substrate. Thermal catalytic decomposition of hydrocarbon has become an active area of research and can be a promising route for the bulk production of CNTs. Fluidised bed reactor is the most widely used reactor for CNT preparation. Scale-up of the reactor is the major challenge.[60] [61]
CVD is a common method for the commercial production of carbon nanotubes. For this purpose, the metal nanoparticles are mixed with a catalyst support such as MgO or Al2O3 to increase the surface area for higher yield of the catalytic reaction of the carbon feedstock with the metal particles. One issue in this synthesis route is the removal of the catalyst support via an acid treatment, which sometimes could destroy the original structure of the carbon nanotubes. However, alternative catalyst supports that are soluble in water have proven effective for nanotube growth.[62]
If a plasma is generated by the application of a strong electric field during the growth process (plasma enhanced chemical vapor deposition), then the nanotube growth will follow the direction of the electric field.[63] By adjusting the geometry of the reactor it is possible to synthesize vertically aligned carbon nanotubes[64] (i.e., perpendicular to the substrate), a morphology that has been of interest to researchers interested in the electron emission from nanotubes. Without the plasma, the resulting nanotubes are often randomly oriented. Under certain reaction conditions, even in the absence of a plasma, closely spaced nanotubes will maintain a vertical growth direction resulting in a dense array of tubes resembling a carpet or forest.
Of the various means for nanotube synthesis, CVD shows the most promise for industrial-scale deposition, because of its price/unit ratio, and because CVD is capable of growing nanotubes directly on a desired substrate, whereas the nanotubes must be collected in the other growth techniques. The growth sites are controllable by careful deposition of the catalyst. In 2007, a team from Meijo University demonstrated a high-efficiency CVD technique for growing carbon nanotubes from camphor.[65] Researchers at Rice University, until recently led by the late Richard Smalley, have concentrated upon finding methods to produce large, pure amounts of particular types of nanotubes. Their approach grows long fibers from many small seeds cut from a single nanotube; all of the resulting fibers were found to be of the same diameter as the original nanotube and are expected to be of the same type as the original nanotube.[66]

Super-growth CVD

Super-growth CVD (water-assisted chemical vapor deposition) process was developed by Kenji Hata, Sumio Iijima and co-workers at AIST, Japan.[67] In this process, the activity and lifetime of the catalyst are enhanced by addition of water into the CVD reactor. Dense millimeter-tall nanotube "forests", aligned normal to the substrate, were produced. The forests growth rate could be expressed, as
 H(t) = {\beta}{\tau}_o ({1 - e^{-t / {\tau}_o}}) .
In this equation, β is the initial growth rate and τo is the characteristic catalyst lifetime.[68]
Their specific surface exceeds 1,000 m2/g (capped) or 2,200 m2/g (uncapped),[69] surpassing the value of 400–1,000 m2/g for HiPco samples. The synthesis efficiency is about 100 times higher than for the laser ablation method. The time required to make SWNT forests of the height of 2.5 mm by this method was 10 minutes in 2004. Those SWNT forests can be easily separated from the catalyst, yielding clean SWNT material (purity >99.98%) without further purification. For comparison, the as-grown HiPco CNTs contain about 5–35%[70] of metal impurities; it is therefore purified through dispersion and centrifugation that damages the nanotubes. The super-growth process avoids this problem. Patterned highly organized single-walled nanotube structures were successfully fabricated using the super-growth technique.
The mass density of super-growth CNTs is about 0.037 g/cm3.[71][72] It is much lower than that of conventional CNT powders (~1.34 g/cm3), probably because the latter contain metals and amorphous carbon.
The super-growth method is basically a variation of CVD. Therefore, it is possible to grow material containing SWNT, DWNTs and MWNTs, and to alter their ratios by tuning the growth conditions.[73] Their ratios change by the thinness of the catalyst. Many MWNTs are included so that the diameter of the tube is wide.[72]
The vertically aligned nanotube forests originate from a "zipping effect" when they are immersed in a solvent and dried. The zipping effect is caused by the surface tension of the solvent and the van der Waals forces between the carbon nanotubes. It aligns the nanotubes into a dense material, which can be formed in various shapes, such as sheets and bars, by applying weak compression during the process. Densification increases the Vickers hardness by about 70 times and density is 0.55 g/cm3. The packed carbon nanotubes are more than 1 mm long and have a carbon purity of 99.9% or higher; they also retain the desirable alignment properties of the nanotubes forest.[74]

Natural, incidental, and controlled flame environments

Fullerenes and carbon nanotubes are not necessarily products of high-tech laboratories; they are commonly formed in such mundane places as ordinary flames,[75] produced by burning methane,[76] ethylene,[77] and benzene,[78] and they have been found in soot from both indoor and outdoor air.[79] However, these naturally occurring varieties can be highly irregular in size and quality because the environment in which they are produced is often highly uncontrolled. Thus, although they can be used in some applications, they can lack in the high degree of uniformity necessary to satisfy the many needs of both research and industry. Recent efforts have focused on producing more uniform carbon nanotubes in controlled flame environments.[80][81][82][83] Such methods have promise for large-scale, low-cost nanotube synthesis, though they must compete with rapidly developing large scale CVD production.

Application related issues


Centrifuge tube with a solution of carbon nanotubes, which were sorted by diameter using density-gradient ultracentrifugation.[84]


Many electronic applications of carbon nanotubes crucially rely on techniques of selectively producing either semiconducting or metallic CNTs, preferably of a certain chirality. Several methods of separating semiconducting and metallic CNTs are known, but most of them are not yet suitable for large-scale technological processes. The most efficient method relies on density-gradient ultracentrifugation, which separates surfactant-wrapped nanotubes by the minute difference in their density. This density difference often translates into difference in the nanotube diameter and (semi)conducting properties.[84] Another method of separation uses a sequence of freezing, thawing, and compression of SWNTs embedded in agarose gel. This process results in a solution containing 70% metallic SWNTs and leaves a gel containing 95% semiconducting SWNTs. The diluted solutions separated by this method show various colors.[85][86] Moreover, SWNTs can be separated by the column chromatography method. Yield is 95% in semiconductor type SWNT and 90% in metallic type SWNT.[87]
In addition to separation of semiconducting and metallic SWNTs, it is possible to sort SWNTs by length, diameter, and chirality. The highest resolution length sorting, with length variation of <10%, has thus far been achieved by size exclusion chromatography (SEC) of DNA-dispersed carbon nanotubes (DNA-SWNT).[88] SWNT diameter separation has been achieved by density-gradient ultracentrifugation (DGU)[89] using surfactant-dispersed SWNTs and by ion-exchange chromatography (IEC) for DNA-SWNT.[90] Purification of individual chiralities has also been demonstrated with IEC of DNA-SWNT: specific short DNA oligomers can be used to isolate individual SWNT chiralities. Thus far, 12 chiralities have been isolated at purities ranging from 70% for (8,3) and (9,5) SWNTs to 90% for (6,5), (7,5) and (10,5)SWNTs.[91] There have been successful efforts to integrate these purified nanotubes into devices, e. g. FETs.[92]
An alternative to separation is development of a selective growth of semiconducting or metallic CNTs. Recently, a new CVD recipe that involves a combination of ethanol and methanol gases and quartz substrates resulting in horizontally aligned arrays of 95–98% semiconducting nanotubes was announced.[93]
Nanotubes are usually grown on nanoparticles of magnetic metal (Fe, Co), which facilitates production of electronic (spintronic) devices. In particular, control of current through a field-effect transistor by magnetic field has been demonstrated in such a single-tube nanostructure.[94]

Current applications

Current use and application of nanotubes has mostly been limited to the use of bulk nanotubes, which is a mass of rather unorganized fragments of nanotubes. Bulk nanotube materials may never achieve a tensile strength similar to that of individual tubes, but such composites may, nevertheless, yield strengths sufficient for many applications. Bulk carbon nanotubes have already been used as composite fibers in polymers to improve the mechanical, thermal and electrical properties of the bulk product.
  • Easton-Bell Sports, Inc. have been in partnership with Zyvex Performance Materials, using CNT technology in a number of their bicycle components—including flat and riser handlebars, cranks, forks, seatposts, stems and aero bars.
  • Zyvex Performance Materials has also built a 54' maritime vessel, the Piranha Unmanned Surface Vessel, as a technology demonstrator for what is possible using CNT technology. CNTs help improve the structural performance of the vessel, resulting in a lightweight 8,000 lb boat that can carry a payload of 15,000 lb over a range of 2,500 miles.[95]
  • Amroy Europe Oy manufactures Hybtonite carbon nanoepoxy resins where carbon nanotubes have been chemically activated to bond to epoxy, resulting in a composite material that is 20% to 30% stronger than other composite materials. It has been used for wind turbines, marine paints and variety of sports gear such as skis, ice hockey sticks, baseball bats, hunting arrows, and surfboards.[96]
Other current applications include:

Potential applications

See also, for last current applications: Timeline of carbon nanotubes

The joining of two carbon nanotubes with different electrical properties to form a diode has been proposed . L Chico et al. Phys Rev Lett 76, 971 (1996)
The strength and flexibility of carbon nanotubes makes them of potential use in controlling other nanoscale structures, which suggests they will have an important role in nanotechnology engineering. The highest tensile strength of an individual multi-walled carbon nanotube has been tested to be is 63 GPa.[18] Carbon nanotubes were found in Damascus steel from the 17th century, possibly helping to account for the legendary strength of the swords made of it.[99][100]

Structural

Because of the carbon nanotube's superior mechanical properties, many structures have been proposed ranging from everyday items like clothes and sports gear to combat jackets and space elevators.[101] However, the space elevator will require further efforts in refining carbon nanotube technology, as the practical tensile strength of carbon nanotubes can still be greatly improved.[20]
For perspective, outstanding breakthroughs have already been made. Pioneering work led by Ray H. Baughman at the NanoTech Institute has shown that single and multi-walled nanotubes can produce materials with toughness unmatched in the man-made and natural worlds.[102][103]
Carbon nanotubes are also a promising material as building blocks in bio-mimetic hierarchical composite materials given their exceptional mechanical properties (~1TPa in modulus, and ~100 GPa in strength). Initial attempts to incorporate CNTs into hierarchical structures led to mechanical properties that were significantly lower than these achievable limits. Windle et al. have used an in situ chemical vapor deposition (CVD) spinning method to produce continuous CNT yarns from CVD grown CNT aerogels.[104][105][106] With this technology, they fabricated CNT yarns with strengths as high as ~9 GPa at small gage lengths of ~1 mm, however, defects resulted in a reduction of specific strength to ~1 GPa at 20 mm gage length.[106][107] Espinosa et al. developed high performance DWNT-polymer composite yarns by twisting and stretching ribbons of randomly oriented bundles of DWNTs thinly coated with polymeric organic compounds. These DWNT-polymer yarns exhibited unusually high energy to failure of ~100 J·g−1 (comparable to one of the toughest natural materials – spider silk[108]), and strength as high as ~1.4 GPa.[109] Effort is ongoing to produce CNT composites that incorporate tougher matrix materials, such as Kevlar, to further improve on the mechanical properties toward those of individual CNTs.
Because of the high mechanical strength of carbon nanotubes, research is being made into weaving them into clothes to create stab-proof and bulletproof clothing. The nanotubes would effectively stop the bullet from penetrating the body, although the bullet's kinetic energy would likely cause broken bones and internal bleeding.[110]

In electrical circuits

Nanotube-based transistors, also known as carbon nanotube field-effect transistors (CNFETs), have been made that operate at room temperature and that are capable of digital switching using a single electron.[111] However, one major obstacle to realization of nanotubes has been the lack of technology for mass production. In 2001 IBM researchers demonstrated how metallic nanotubes can be destroyed, leaving semiconducting ones behind for use as transistors. Their process is called "constructive destruction," which includes the automatic destruction of defective nanotubes on the wafer.[112] This process, however, only gives control over the electrical properties on a statistical scale.
The potential of carbon nanotubes was demonstrated in 2003 when room-temperature ballistic transistors with ohmic metal contacts and high-k gate dielectric were reported, showing 20–30x higher ON current than state-of-the-art Si MOSFETs. This presented an important advance in the field as CNT was shown to potentially outperform Si. At the time, a major challenge was ohmic metal contact formation. In this regard, palladium, which is a high-work function metal was shown to exhibit Schottky barrier-free contacts to semiconducting nanotubes with diameters >1.7 nm.[113][114]
The first nanotube integrated memory circuit was made in 2004. One of the main challenges has been regulating the conductivity of nanotubes. Depending on subtle surface features a nanotube may act as a plain conductor or as a semiconductor. A fully automated method has however been developed to remove non-semiconductor tubes.[115]
Another way to make carbon nanotube transistors has been to use random networks of them. By doing so one averages all of their electrical differences and one can produce devices in large scale at the wafer level.[116] This approach was first patented by Nanomix Inc.[117](date of original application June 2002[118] ). It was first published in the academic literature by the United States Naval Research Laboratory in 2003 through independent research work. This approach also enabled Nanomix to make the first transistor on a flexible and transparent substrate.[119][120]
Large structures of carbon nanotubes can be used for thermal management of electronic circuits. An approximately 1 mm–thick carbon nanotube layer was used as a special material to fabricate coolers, this materials has very low density, ~20 times lower weight than a similar copper structure, while the cooling properties are similar for the two materials.[121]
Overall, incorporating carbon nanotubes as transistors into logic-gate circuits with densities comparable to modern CMOS technology has not yet been demonstrated.

As electrical cables and wires

Wires for carrying electrical current may be fabricated from pure nanotubes and nanotube-polymer composites. Recently small wires have been fabricated with specific conductivity exceeding copper and aluminum[122][123]; these cables are the highest conductivity carbon nanotube and also highest conductivity non-metal cables.

As paper batteries

A paper battery is a battery engineered to use a paper-thin sheet of cellulose (which is the major constituent of regular paper, among other things) infused with aligned carbon nanotubes.[124] The nanotubes act as electrodes; allowing the storage devices to conduct electricity. The battery, which functions as both a lithium-ion battery and a supercapacitor, can provide a long, steady power output comparable to a conventional battery, as well as a supercapacitor’s quick burst of high energy—and while a conventional battery contains a number of separate components, the paper battery integrates all of the battery components in a single structure, making it more energy efficient.[citation needed]

Solar cells

Solar cells developed at the New Jersey Institute of Technology use a carbon nanotube complex, formed by a mixture of carbon nanotubes and carbon buckyballs (known as fullerenes) to form snake-like structures. Buckyballs trap electrons, although they can't make electrons flow. Add sunlight to excite the polymers, and the buckyballs will grab the electrons. Nanotubes, behaving like copper wires, will then be able to make the electrons or current flow.[125]

Ultracapacitors

MIT Laboratory for Electromagnetic and Electronic Systems uses nanotubes to improve ultracapacitors. The activated charcoal used in conventional ultracapacitors has many small hollow spaces of various size, which create together a large surface to store electric charge. But as charge is quantized into elementary charges, i.e. electrons, and each such elementary charge needs a minimum space, a significant fraction of the electrode surface is not available for storage because the hollow spaces are not compatible with the charge's requirements. With a nanotube electrode the spaces may be tailored to size—few too large or too small—and consequently the capacity should be increased considerably.[126]

Medical

In the Kanzius cancer therapy, single-walled carbon nanotubes are inserted around cancerous cells, then excited with radio waves, which causes them to heat up and kill the surrounding cells.
Researchers at Rice University, Radboud University Nijmegen Medical Centre and University of California, Riverside have shown that carbon nanotubes and their polymer nanocomposites are suitable scaffold materials for bone cell proliferation [127][128] and bone formation.[129][130]

Other applications


Aligned nanotubes are preferred for many applications.

Carbon nanotubes have been implemented in nanoelectromechanical systems, including mechanical memory elements (NRAM being developed by Nantero Inc.) and nanoscale electric motors (see Nanomotor or Nanotube nanomotor).
In May 2005, Nanomix Inc. placed on the market a hydrogen sensor that integrated carbon nanotubes on a silicon platform. Since then, Nanomix has been patenting many such sensor applications, such as in the field of carbon dioxide, nitrous oxide, glucose, DNA detection, etc.
Eikos Inc of Franklin, Massachusetts and Unidym Inc. of Silicon Valley, California are developing transparent, electrically conductive films of carbon nanotubes to replace indium tin oxide (ITO). Carbon nanotube films are substantially more mechanically robust than ITO films, making them ideal for high-reliability touchscreens and flexible displays. Printable water-based inks of carbon nanotubes are desired to enable the production of these films to replace ITO.[131] Nanotube films show promise for use in displays for computers, cell phones, PDAs, and ATMs.
A nanoradio, a radio receiver consisting of a single nanotube, was demonstrated in 2007. In 2008 it was shown that a sheet of nanotubes can operate as a loudspeaker if an alternating current is applied. The sound is not produced through vibration but thermoacoustically.[132]
A flywheel made of carbon nanotubes could be spun at extremely high velocity on a floating magnetic axis in a vacuum, and potentially store energy at a density approaching that of conventional fossil fuels. Since energy can be added to and removed from flywheels very efficiently in the form of electricity, this might offer a way of storing electricity, making the electrical grid more efficient and variable power suppliers (like wind turbines) more useful in meeting energy needs. The practicality of this depends heavily upon the cost of making massive, unbroken nanotube structures, and their failure rate under stress.
Carbon nanotube springs have the potential to indefinitely store elastic potential energy at ten times the density of lithium-ion batteries with flexible charge and discharge rates and extremely high cycling durability.
Ultra-short SWNTs (US-tubes) have been used as nanoscaled capsules for delivering MRI contrast agents in vivo.[133]
Nitrogen-doped carbon nanotubes may replace platinum catalysts used to reduce oxygen in fuel cells. A forest of vertically-aligned nanotubes can reduce oxygen in alkaline solution more effectively than platinum, which has been used in such applications since the 1960s. The nanotubes have the added benefit of not being subject to carbon monoxide poisoning.[134]

Optical properties of carbon nanotubes


Within materials science, the optical properties of carbon nanotubes refer specifically to the absorption, photoluminescence, and Raman spectroscopy of carbon nanotubes. Spectroscopic methods offer the possibility of quick and non-destructive characterization of relatively large amounts of carbon nanotubes. There is a strong demand for such characterization from the industrial point of view: numerous parameters of the nanotube synthesis can be changed, intentionally or unintentionally, to alter the nanotube quality. As shown below, optical absorption, photoluminescence and Raman spectroscopies allow quick and reliable characterization of this "nanotube quality" in terms of non-tubular carbon content, structure (chirality) of the produced nanotubes, and structural defects. Those features determine nearly any other properties such as optical, mechanical, and electrical properties.
Carbon nanotubes are unique "one dimensional systems" which can be envisioned as rolled single sheets of graphite (or more precisely graphene). This rolling can be done at different angles and curvatures resulting in different nanotube properties. The diameter typically varies in the range 0.4–40 nm (i.e. "only" ~100 times), but the length can vary ~10,000 times reaching 18.5 cm.[1] Thus the nanotube aspect ratio, or the length-to-diameter ratio, can be as high as 132,000,000:1,[2] which is unequalled by any other material. Consequently, all the properties of the carbon nanotubes relative to those of typical semiconductors are extremely anisotropic (directionally dependent) and tunable.
Whereas mechanical, electrical and electrochemical (supercapacitor) properties of the carbon nanotubes are well established and have immediate applications, the practical use of optical properties is yet unclear. The aforementioned tunability of properties is potentially useful in optics and photonics. In particular, light-emitting diodes (LEDs)[3][4] and photo-detectors[5] based on a single nanotube have been produced in the lab. Their unique feature is not the efficiency, which is yet relatively low, but the narrow selectivity in the wavelength of emission and detection of light and the possibility of its fine tuning through the nanotube structure. In addition, bolometer[6] and optoelectronic memory[7] devices have been realised on ensembles of single-walled carbon nanotubes.

Terminology

This article uses the following abbreviations:
  • Carbon nanotube (CNT)
  • Single wall carbon nanotube (SWCNT)
  • Multiwall carbon nanotube (MWCNT)
However, C is often omitted in scientific literature,[8] so NT, SWNT and MWNT are more commonly used. Also, "wall" is often exchanged with "walled".

Electronic structure of carbon nanotube


The (n, m) nanotube naming scheme[8][9] can be thought of as a vector (Ch) in an infinite graphene sheet that describes how to "roll up" the graphene sheet to make the nanotube. T denotes the tube axis, and a1 and a2 are the unit vectors of graphene in real space.

Armchair nanotube

Zigzag nanotube
A single-wall carbon nanotube can be imagined as graphene sheet rolled at a certain "chiral" angle with respect to a plane perpendicular to the tube's long axis. Consequently, SWCNT can be defined by its diameter and chiral angle. The chiral angle can range from 0 to 30 degrees.
However, more conveniently, a pair of indices (n, m) is used instead. The indices refer to equally long unit vectors at 60° angles to each other across a single 6-member carbon ring. Taking the origin as carbon number 1, the a1 unit vector may be considered the line drawn from carbon 1 to carbon 3, and the a2 unit vector is then the line drawn from carbon 1 to carbon 5. (See the upper right corner of the diagram at right.) To visualize a CNT with indices (n, m), draw n a1 unit vectors across the graphene sheet, then draw m a2 unit vectors at a 60° angle to the a1 vectors, then add the vectors together. The line representing the sum of the vectors will define the circumference of the CNT along the plane perpendicular to its long axis, connecting one end to the other.[8][9][10] In the diagram at right, Ch is a (4, 2) vector: the sum of 4 unit vectors from the origin directly to the right, then 2 unit vectors at a 60° angle down and to the right.
Tubes having n = m (chiral angle = 30°) are called "armchair" and those with m = 0 (chiral angle = 0°) "zigzag". Those indices uniquely determine whether CNT is a metal, semimetal or semiconductor, as well as its band gap: when |m – n| = 3k (k is integer), the tube is metallic; but if |m – n| = 3k ± 1, the tube is semiconducting. The nanotube diameter d is related to m and n as
 d = \frac{a}{\pi} \sqrt{(n^2 + nm + m^2)}.
In this equation, a = 0.246 nm is the magnitude of either unit vector a1 or a2.
The situation in multi-wall CNTs is complicated as their properties are determined by contribution of all individual shells; those shells have different structures, and, because of the synthesis, are usually more defective than SWCNTs. Therefore, optical properties of MWCNTs will not be considered here.

Van Hove singularities

SSPN41.PNG

A bulk 3D material (blue) has continuous DOS, but a 1D wire (green) has Van Hove singularities.
Optical properties of carbon nanotubes derive from electronic transitions within one-dimensional density of states (DOS). A typical feature of one-dimensional crystals is that their DOS is not a continuous function of energy, but it descends gradually and then increases in a discontinuous spike. In contrast, three-dimensional materials have continuous DOS. The sharp peaks found in one-dimensional materials are called Van Hove singularities.
Van Hove singularities result in the following remarkable optical properties of carbon nanotubes:
  • Optical transitions occur between the v1 − c1, v2 − c2, etc., states of semiconducting or metallic nanotubes and are traditionally labeled as S11, S22, M11, etc., or, if the "conductivity" of the tube is unknown or unimportant, as E11, E22, etc. Crossover transitions c1 − v2, c2 − v1, etc., are dipole-forbidden and thus are extremely weak, but they were possibly observed using cross-polarized optical geometry.[11]
  • The energies between the Van Hove singularities depend on the nanotube structure. Thus by varying this structure, one can tune the optoelectronic properties of carbon nanotube. Such fine tuning has been experimentally demonstrated using UV illumination of polymer-dispersed CNTs.[12]
  • Optical transitions are rather sharp (~10 meV) and strong. Consequently, it is relatively easy to selectively excite nanotubes having certain (n, m) indices, as well as to detect optical signals from individual nanotubes.

Kataura plot


In this Kataura plot, the energy of an electronic transition decreases as the diameter of the nanotube increases.
The band structure of carbon nanotubes having certain (n, m) indexes can be easily calculated.[13] A theoretical graph based on this calculations was designed in 1999 by Hiromichi Kataura to rationalize experimental findings. A Kataura plot relates the nanotube diameter and its bandgap energies for all nanotubes in a diameter range.[14] The oscillating shape of every branch of the Kataura plot reflects the intrinsic strong dependence of the SWCNT properties on the (n, m) index rather than on its diameter. For example, (10, 0) and (8, 3) tubes have almost the same diameter, but very different properties: the former is a metal, but the latter is semiconductor.

Optical absorption


Optical absorption spectrum from dispersed single-wall carbon nanotubes
Optical absorption in carbon nanotubes differs from absorption in conventional 3D materials by presence of sharp peaks (1D nanotubes) instead of an absorption threshold followed by an absorption increase (most 3D solids). Absorption in nanotubes originates from electronic transitions from the v2 to c2 (energy E22) or v1 to c1 (E11) levels, etc.[8][14] The transitions are relatively sharp and can be used to identify nanotube types. Note that the sharpness deteriorates with increasing energy, and that many nanotubes have very similar E22 or E11 energies, and thus significant overlap occurs in absorption spectra. This overlap is avoided in photoluminescence mapping measurements (see below), which instead of a combination of overlapped transitions identifies individual (E22, E11) pairs.[15][16]
Interactions between nanotubes, such as bundling, broaden optical lines. While bundling strongly affects photoluminescence, it has much weaker effect on optical absorption and Raman scattering. Consequently, sample preparation for the latter two techniques is relatively simple.
Optical absorption is routinely used to quantify quality of the carbon nanotube powders.[17] The spectrum is analyzed in terms of intensities of nanotube-related peaks, background and pi-carbon peak; the latter two mostly originate from non-nanotube carbon.

Carbon nanotubes as a black body

An ideal black body should have emissivity or absorbance of 1.0, which is difficult to attain in practice, especially in a wide spectral range. Vertically aligned "forests" of single-wall carbon nanotubes can have absorbances of 0.98–0.99 from the far-ultraviolet (200 nm) to far-infrared (200 μm) wavelengths. Super black, a coating based on chemically etched nickel-phosphorus alloy, is another material approaching the absorption of 1.0.
These SWNT forests (buckypaper) were grown by the super-growth CVD method to about 10 μm height. Two factors could contribute to strong light absorption by these structures: (i) a distribution of CNT chiralities resulted in various bandgaps for individual CNTs. Thus a compound material was formed with broadband absorption. (ii) Light might be trapped in those forests due to multiple reflections.[18][19][20]
Reflectance measurements[21]

UV-to-near IR Near-to-mid IR Mid-to-far IR
Wavelength, μm 0.2-2 2-20 25-200
Incident angle, ° 8 5 10
Reflection Hemispherical-directional Hemispherical-directional Specular
Reference White reflectance standard Gold mirror Aluminum mirror
Average reflectance 0.0160 0.0097 0.0017
Standard deviation 0.0048 0.0041 0.0027

Luminescence


Photoluminescence map from single-wall carbon nanotubes. (n, m) indexes identify certain semiconducting nanotubes. Note that PL measurements do not detect nanotubes with n = m or m = 0.

Excitation mechanism

Photoluminescence (PL) is one of the important tools for nanotube characterization. The excitation of PL usually occurs as follows: an electron in a nanotube absorbs excitation light via S22 transition, creating an electron-hole pair (exciton). Both electron and hole rapidly relax (via phonon-assisted processes) from c2 to c1 and from v2 to v1 states, respectively. Then they recombine through a c1 − v1 transition resulting in light emission.
No excitonic luminescence can be produced in metallic tubes — electron can be excited, thus resulting in optical absorption, but the hole is immediately filled by another electron out of many available in metal. Therefore no exciton is produced.

Salient properties

  • Photoluminescence from SWCNT, as well as optical absorption and Raman scattering, is linearly polarized along the tube axis. This allows monitoring of the SWCNTs orientation without direct microscopic observation.
  • PL is quick: relaxation typically occurs within 100 picoseconds.[22]
  • PL efficiency is usually low (~0.01%),[22] however, there is room for enhancement, e.g., through improving the structural quality of the nanotubes and clever nanotube isolation strategies. For example, the efficiency of 3% has been reported in nanotubes sorted by diameter and length through gradient centrifugation,[23] and it has been further increased to 20% by optimizing the procedure of isolating individual nanotubes in solution.[24]
  • The spectral range of PL is rather wide. Emission wavelength can vary between 0.8 and 2.1 micrometers depending on the nanotube structure.[15][16]
  • Interaction between nanotubes or between nanotube and another material (e.g., substrate) quenches PL. For this reason, no PL is observed in multi-wall carbon nanotubes. PL from double-wall carbon nanotubes strongly depends on how they were prepared: CVD grown DWCNTs show emission both from inner and outer shells.[15][16] However, DWCNTs produced by encapsulating fullerenes into SWCNTs and annealing show PL only from the outer shells.[25] Isolated SWCNTs lying on the substrate show extremely weak PL which has been detected in few studies only.[26] Detachment of the tubes from the substrate drastically increases PL.
  • Position of the (S22, S11) PL peaks depends slightly (within 2%) on the nanotube environment (air, dispersant, etc.). However, the shift depends on the (n, m) index, and thus the whole PL map not only shifts, but also warps upon changing the CNT medium.

Applications

Because of low efficiency, no commercial application of PL from pure carbon nanotubes is viable yet. However, PL is widely used to deduce (n, m) indices: first nanotubes are isolated (dispersed) using an appropriate chemical agent ("dispersant") to reduce the intertube quenching. Then PL is measured, scanning both the excitation and emission energies and thereby producing a PL map. The ovals in the map define (S22, S11) pairs, which unique identify (n, m) index of a tube. The data of Weisman and Bachilo are conventionally used for the identification.[27]

Sensitization

Optical properties, including the PL efficiency, can be modified by encapsulating organic dyes (carotene, lycopene, etc.) inside the tubes.[28][29] Efficient energy transfer occurs between the encapsulated dye and nanotube — light is efficiently absorbed by the dye and without significant loss is transferred to the SWCNT. Thus potentially, optical properties of a carbon nanotube can be controlled by encapsulating certain molecule inside it. Besides, encapsulation allows isolation and characterization of organic molecules which are unstable under ambient conditions. For example, Raman spectra are extremely difficult to measure from dyes because of their strong PL (efficiency close to 100%). However, encapsulation of dye molecules inside SWCNTs completely quenches dye PL, thus allowing measurement and analysis of their Raman spectra.[30]

Cathodoluminescence

Cathodoluminescence (CL) — light emission excited by electron beam — is a process commonly observed in TV screens. An electron beam can be finely focused and scanned across the studied material. This technique is widely used to study defects in semiconductors and nanostructures with nanometer-scale spatial resolution.[31] It would be beneficial to apply this technique to carbon nanotubes. However, no reliable CL, i.e. sharp peaks assignable to certain (n, m) indices, has been detected from carbon nanotubes yet.

Electroluminescence

If appropriate electrical contacts are attached to a nanotube, electron-hole pairs (excitons) can be generated by injecting electrons and holes from the contacts. Subsequent exciton recombination results in electroluminescence (EL). Electroluminescent devices have been produced from single nanotubes.[3][4][32]

Raman scattering


Raman spectrum of single-wall carbon nanotubes
Raman spectroscopy has good spatial resolution (~0.5 micrometers) and sensitivity (single nanotubes); it requires only minimal sample preparation and is rather informative. Consequently, Raman spectroscopy is probably the most popular technique of carbon nanotube characterization. Raman scattering in SWCNTs is resonant, i.e., only those tubes are probed which have one of the bandgaps equal to the exciting laser energy.[33][34] Several scattering modes dominate the SWCNT spectrum, as discussed below.
Similar to photoluminescence mapping, the energy of the excitation light can be scanned in Raman measurements, thus producing Raman maps.[33] Those maps also contain oval-shaped features uniquely identifying (n, m) indices. Contrary to PL, Raman mapping detects not only semiconducting but also metallic tubes, and it is less sensitive to nanotube bundling than PL. However, requirement of a tunable laser and a dedicated spectrometer is a strong technical impediment.

Radial breathing mode

Radial breathing mode (RBM) corresponds to radial expansion-contraction of the nanotube. Therefore, its frequency νRBM (in cm−1) depends on the nanotube diameter d (in nanometers) and can be estimated[33][34] as νRBM = 223/d + 10, which is very useful in deducing the CNT diameter from the RBM position. Typical RBM range is 100–350 cm−1. If RBM intensity is particularly strong, its weak second overtone can be observed at double frequency.

Bundling mode

The bundling mode is a special form of RBM supposedly originating from collective vibration in a bundle of SWCNTs.[35]

G mode

Another very important mode is the G mode (G from graphite). This mode corresponds to planar vibrations of carbon atoms and is present in most graphite-like materials.[10] G band in SWCNT is shifted to lower frequencies relative to graphite (1580 cm−1) and is split into several peaks. The splitting pattern and intensity depend on the tube structure and excitation energy; they can be used, though with much lower accuracy compared to RBM mode, to estimate the tube diameter and whether the tube is metallic or semiconducting.

D mode

D mode is present in all graphite-like carbons and originates from structural defects.[10] Therefore, the ratio of the G/D modes is conventionally used to quantify the structural quality of carbon nanotubes. High-quality nanotubes have this ratio significantly higher than 100.

G' mode

The name of this mode is misleading: it is given because in graphite, this mode is usually the second strongest after the G mode. However, it is actually the second overtone of the defect-induced D mode (and thus should logically be named D'). Its intensity is stronger than that of the D mode due to different selection rules.[10] In particular, D mode is forbidden in the ideal nanotube and requires a structural defect, providing a phonon of certain angular momentum, to be induced. In contrast, G' mode involves a "self-annihilating" pair of phonons and thus does not require defects. The spectral position of G' mode depends on diameter, so it can be used roughly to estimate the SWCNT diameter.[16] In particular, G' mode is a doublet in double-wall carbon nanotubes, but the doublet is often unresolved due to line broadening.
Other overtones, such as a combination of RBM+G mode at ~1750 cm−1, are frequently seen in CNT Raman spectra. However, they are less important and are not considered here.

Anti-Stokes scattering

All the above Raman modes can be observed both as Stokes and anti-Stokes scattering. As mentioned above, Raman scattering from CNTs is resonant in nature, i.e. only tubes whose band gap energy is similar to the laser energy are excited. The difference between those two energies, and thus the band gap of individual tubes, can be estimated from the intensity ratio of the Stokes/anti-Stokes lines.[33][34] This estimate however relies on the temperature factor (Boltzmann factor), which is often miscalculated - focused laser beam is used in the measurement, which can locally heat the nanotubes without changing the overall temperature of the studied sample.

Rayleigh scattering

Carbon nanotubes have very large aspect ratio, i.e., their length is much larger than their diameter. Consequently, as expected from the classical electromagnetic theory, elastic light scattering (or Rayleigh scattering) by straight CNTs has anisotropic angular dependence, and from its spectrum, the band gaps of individual nanotubes can be deduced.[36][37]
Another manifestation of Rayleigh scattering is the "antenna effect", an array of nanotubes standing on a substrate has specific angular and spectral distributions of reflected light, and both those distributions depend on the nanotube length.[38]

Discovery

A 2006 editorial written by Marc Monthioux and Vladimir Kuznetsov in the journal Carbon described the interesting and often-misstated origin of the carbon nanotube. A large percentage of academic and popular literature attributes the discovery of hollow, nanometer-size tubes composed of graphitic carbon to Sumio Iijima of NEC in 1991.[135]
In 1952 L. V. Radushkevich and V. M. Lukyanovich published clear images of 50 nanometer diameter tubes made of carbon in the Soviet Journal of Physical Chemistry.[136] This discovery was largely unnoticed, as the article was published in the Russian language, and Western scientists' access to Soviet press was limited during the Cold War. It is likely that carbon nanotubes were produced before this date, but the invention of the transmission electron microscope (TEM) allowed direct visualization of these structures.
Carbon nanotubes have been produced and observed under a variety of conditions prior to 1991. A paper by Oberlin, Endo, and Koyama published in 1976 clearly showed hollow carbon fibers with nanometer-scale diameters using a vapor-growth technique.[137] Additionally, the authors show a TEM image of a nanotube consisting of a single wall of graphene. Later, Endo has referred to this image as a single-walled nanotube.[138]
In 1979, John Abrahamson presented evidence of carbon nanotubes at the 14th Biennial Conference of Carbon at Pennsylvania State University. The conference paper described carbon nanotubes as carbon fibers that were produced on carbon anodes during arc discharge. A characterization of these fibers was given as well as hypotheses for their growth in a nitrogen atmosphere at low pressures.[139]
In 1981, a group of Soviet scientists published the results of chemical and structural characterization of carbon nanoparticles produced by a thermocatalytical disproportionation of carbon monoxide. Using TEM images and XRD patterns, the authors suggested that their “carbon multi-layer tubular crystals” were formed by rolling graphene layers into cylinders. They speculated that by rolling graphene layers into a cylinder, many different arrangements of graphene hexagonal nets are possible. They suggested two possibilities of such arrangements: circular arrangement (armchair nanotube) and a spiral, helical arrangement (chiral tube).[140]
In 1987, Howard G. Tennett of Hyperion Catalysis was issued a U.S. patent for the production of "cylindrical discrete carbon fibrils" with a "constant diameter between about 3.5 and about 70 nanometers..., length 102 times the diameter, and an outer region of multiple essentially continuous layers of ordered carbon atoms and a distinct inner core...."[141]
Iijima's discovery of multi-walled carbon nanotubes in the insoluble material of arc-burned graphite rods in 1991[142] and Mintmire, Dunlap, and White's independent prediction that if single-walled carbon nanotubes could be made, then they would exhibit remarkable conducting properties [143] helped create the initial buzz that is now associated with carbon nanotubes. Nanotube research accelerated greatly following the independent discoveries[144][145] by Bethune at IBM[146] and Iijima at NEC of single-walled carbon nanotubes and methods to specifically produce them by adding transition-metal catalysts to the carbon in an arc discharge. The arc discharge technique was well-known to produce the famed Buckminster fullerene on a preparative scale,[147] and these results appeared to extend the run of accidental discoveries relating to fullerenes. The original observation of fullerenes in mass spectrometry was not anticipated,[148] and the first mass-productioBlogger: Fisika Teori dan Terapan - Edit postn technique by Krätschmer and Huffman was used for several years before realizing that it produced fullerenes.[147]
The discovery of nanotubes remains a contentious issue. Many believe that Iijima's report in 1991 is of particular importance because it brought carbon nanotubes into the awareness of the scientific community as a whole.[135]

Potential applications of carbon nanotubes


Carbon nanotubes have valuable qualities as structural materials. Potential uses include:
  • Textiles—CNT can make waterproof and/or tear-resistant fabrics
  • Body armor—MIT is working on combat jackets that use CNT fibers to stop bullets and to monitor the condition of the wearer.[1] Cambridge University developed the fibres and licensed a company to make them.[2]
  • Concrete—CNT in concrete increase its tensile strength, and halt crack propagation.[3]
  • Polyethylene—Adding CNT to polyethylene can increase the polymer's elastic modulus by 30%.
  • Sports equipment—Stronger and lighter tennis rackets, bicycle parts, golf balls, golf clubs, and baseball bats.
  • Space elevator—CNT are under investigation as possible components of the tether up which a space elevator can climb. This requires tensile strengths of more than about 70 GPa.
  • synthetic muscles: Due to their high contraction/extension ratio given an electric current, CNTs are ideal for synthetic muscle.[4]
  • High tensile strength fibers—Fibers produced with polyvinyl alcohol required 600 J/g to break.[5] In comparison, the bullet-resistant fiber Kevlar fails at 27–33 J/g.
  • Bridges—CNT may be able to replace steel in suspension and other bridges.
  • Flywheels—The high strength/weight ratio enables very high rotational speeds.
  • Carbon nanotube springs—Single-walled carbon nanotubes aligned in parallel can be elastically stretched for an energy density 10 times greater than that of current lithium-ion batteries, with the additional advantages of long cycling durability, temperature insensitivity, no spontaneous dischange, and arbitrary discharge rate.
  • Fire protection—Thin layers of buckypaper can significantly improve fire resistance due to the efficient reflection of heat by the dense, compact layer of CNT or carbon fibers.[6]

Electromagnetic

CNT can be fabricated as electrical conductors, insulators, and semiconductors. Applications include:
  • Artificial muscles—CNT's have sufficient contractility to make them candidates to replace muscle tissue.[7]
  • Buckypaper—Thin nanotube sheets are 250 times stronger than steel and 10 times lighter and could be used as a heat sink for chipboards, a backlight for LCD screens or as a faraday cage to protect electrical devices/aeroplanes.
  • Chemical nanowires—CNTs can be used to produce nanowires of other elements/molecules, such as gold or zinc oxide. These nanowires in turn can be used to cast nanotubes of other chemicals, such as gallium nitride. These can have very different properties from CNTs—for example, gallium nitride nanotubes are hydrophilic, while CNTs are hydrophobic, giving them possible uses in organic chemistry.
  • Conductive films— Canatu [8] of Helsinki, Finland, Eikos Inc of Franklin, Massachusetts and Unidym Inc.[9] of Silicon Valley are developing transparent, electrically conductive CNT films and NanoBuds to replace indium tin oxide (ITO) in LCDs, touch screens, and photovoltaic devices. Nanotube films show promise for use in displays for computers, cell phones, Personal digital assistants, and automated teller machines.
  • Electric motor brushes—Conductive CNTs are used in brushes for commercial electric motors. They replace traditional carbon black. The nanotubes improve electrical and thermal conductivity because they stretch through the plastic matrix of the brush. This permits the carbon filler to be reduced from 30% down to 3.6%, so that more matrix is present in the brush. Nanotube composite motor brushes are better-lubricated (from the matrix), cooler-running (both from better lubrication and superior thermal conductivity), less brittle (more matrix, and fiber reinforcement), stronger and more accurately moldable (more matrix). Since brushes are a critical failure point in electric motors, and also don't need much material, they became economical before almost any other application.
  • Light bulb filament: alternative to tungsten filaments in incandescent lamps.
  • Magnets—Multi-walled nanotubes (MWNT coated with magnetite can generate strong magnetic fields.)
  • Optical ignition—A layer of 29% iron enriched single-walled nanotubes (SWNT) is placed on top of a layer of explosive material such as PETN, and can be ignited with a regular camera flash.[10]
  • Solar cells—GE's CNT diode exploits a photovoltaic effect. Nanotubes can replace ITO in some solar cells to act as a transparent conductive film in solar cells to allow light to pass to the active layers and generate photocurrent.
  • Superconductor—Nanotubes have been shown to be superconducting at low temperatures.[11]
  • Ultracapacitors—MIT is researching the use of nanotubes bound to the charge plates of capacitors in order to dramatically increase the surface area and therefore energy storage ability.[12]
  • Displays—CNTs can be used as extremely fine electron guns, which could be used as miniature cathode ray tubes in thin high-brightness, low-energy, low-weight displays. This type of display would consist of a group of many tiny CRTs, each providing the electrons to hit the phosphor of one pixel, instead of having one giant CRT whose electrons are aimed using electric and magnetic fields. These displays are known as field emission displays (FEDs).
  • Transistor—CNT transistors have been developed at Delft, IBM, and NEC.
  • Electromagnetic antenna—CNTs can act as antennas for radios and other electromagnetic devices.[13]

Electroacoustic

Chemical

  • Desalination— water molecules can be separated from salt by forcing them through networks of carbon nanotubes, which require far lower pressures than conventional reverse osmosis methods [15]
  • Air pollution filter—CNT membranes can filter carbon dioxide from power plant emissions.
  • Biotech container—CNT can be filled with biological molecules, aiding biotechnology.
  • Hydrogen storage—CNT have the potential to store between 4.2 and 65% hydrogen by weight. If they can be mass produced economically, 13.2 litres (2.9 imp gal; 3.5 US gal) of CNT could contain the same amount of energy as a 50 litres (11 imp gal; 13 US gal) gasoline tank. See Hydrogen Economy.[citation needed]

Mechanical

 Electrical circuits

A nanotube formed by joining two nanotubes of different diameters end to end can act as a diode, suggesting the possibility of constructing computer circuits entirely of nanotubes. Because of their good thermal transmission properties, CNT can potentially dissipate heat from computer chips. The longest electricity conducting circuit is a fraction of an inch long.[18]
Fabrication difficulties are major hurdles for CNT. Standard IC fabrication processes use chemical vapor deposition to add layers to a wafer. CNT can so far not be mass produced using such techniques.
Researchers can manipulate nanotubes one-by-one with the tip of an atomic force microscope in a time-consuming process. Using standard fabrication techniques would still require designers to position one end of the nanotube. During the deposition process, an electric field can potentially direct the growth of the nanotubes, which tend to grow along the field lines from negative to positive polarity. Another technique for self-assembly uses chemical or biological techniques to move CNT in solution to determinate places on a substrate.
Even if nanotubes can be precisely positioned, engineers have been unable to control the types (conducting, semiconducting, SWNT, MWNT) of nanotubes that appear.

Interconnects

Metallic carbon nanotubes have aroused research interest for their applicability as very-large-scale integration (VLSI) interconnects because of their high thermal stability, high thermal conductivity and large current carrying capacity.[19][20][21][22][23][24] An isolated CNT can carry current densities in excess of 1000 MA/sq-cm without damage even at an elevated temperature of 250 °C (482 °F), eliminating electromigration reliability concerns that plague Cu interconnects. Recent modeling work comparing the two has shown that CNT bundle interconnects can potentially offer advantages over copper.[25] Recent experiments demonstrated resistances as low as 20 Ohms using different architectures,[26] detailed conductance measurements over a wide temperature range were shown to agree with theory for a strongly disordered quasi-one-dimensional conductor.
Hybrid interconnects that employ CNT vias in tandem with copper interconnects offers advantages from a reliability/thermal-management perspective.

Transistors

Semiconducting CNTs have been used to fabricate field effect transistors (CNTFETs), which show promise due to their superior electrical characteristics over silicon based MOSFETs. Since the electron mean free path in SWCNTs can exceed 1 micrometer, long channel CNTFETs exhibit near-ballistic transport characteristics, resulting in high speed devices. CNT devices are projected to operate in the frequency range of hundreds of Gigaherz. Recent work detailing the advantages and disadvantages of various forms of CNTFETs have also shown that tunneling CNTFET offers better characteristics compared to other CNTFET structures. This device has been found to be superior in terms of subthreshold slope - a very important property for low power applications.[27][28][29][30][31][32]
Nanotubes are usually grown on nanoparticles of magnetic metal (Fe, Co) that facilitates production of electronic (spintronic) devices. In particular control of current through a field-effect transistor by magnetic field has been demonstrated in such a single-tube nanostructure.[33]

Electronic design and design automation

Although CNT devices and interconnects separately have been shown to be promising in their own respects, there have been few efforts to combine them in a realistic circuit. Most CNTFET structures employ the silicon substrate as a back gate. Applying different back gate voltages might become a concern when designing large circuits out of these elements. Several top-gated structures have also been demonstrated, which can alleviate this concern. Recently, a fully integrated logic circuit built on a single nanotube was reported. This circuit employs a back-gate. Several process-related challenges need to be addressed before CNT-based devices and interconnects can enter mainstream VLSI manufacturing. Remaining problems include purification, separation, control over length, chirality and desired alignment, low thermal budget and high contact resistance. Innovative ideas have been proposed to build practical transistors out of nano-networks. Since lack of control on chirality produces a mix of metallic as well as semi-conducting CNTs from any fabrication process and it is difficult to control the growth direction of the CNTs, easily-produced random arrays of SWCNTs have been proposed to build thin film transistors. This idea can be further exploited to build practical CNT based transistors and circuits without the need for precise growth and assembly.

Medicine

Research at University of California, Riverside has shown that carbon nanotubes are suitable scaffold materials for osteoblast proliferation and bone formation.[34]

Carbon nanotubes in photovoltaics

From Wikipedia, the free encyclopedia
Jump to: navigation, search
Organic photovoltaic devices (OPVs) are fabricated from thin films of organic semiconductors, such as polymers and small-molecule compounds, and are typically on the order of 100 nm thick. Because polymer based OPVs can be made using a coating process such as spin coating or inkjet printing, they are an attractive option for inexpensively covering large areas as well as flexible plastic surfaces. A promising low cost alternative to silicon solar cells, there is a large amount of research being dedicated throughout industry and academia towards developing OPVs and increasing their power conversion efficiency.[1]

Carbon nanotube composites in the photoactive layer

Combining the physical and chemical characteristics of conjugated polymers with the high conductivity along the tube axis of carbon nanotubes (CNTs) provides a great deal of incentive to disperse CNTs into the photoactive layer in order to obtain more efficient OPV devices. The interpenetrating bulk donor–acceptor heterojunction in these devices can achieve charge separation and collection because of the existence of a bicontinuous network. Along this network, electrons and holes can travel toward their respective contacts through the electron acceptor and the polymer hole donor. Photovoltaic efficiency enhancement is proposed to be due to the introduction of internal polymer/nanotube junctions within the polymer matrix. The high electric field at these junctions can split up the excitons, while the single-walled carbon nanotube (SWCNT) can act as a pathway for the electrons.[2]
The dispersion of CNTs in a solution of an electron donating conjugated polymer is perhaps the most common strategy to implement CNT materials into OPVs. Generally poly(3-hexylthiophene) (P3HT) or poly(3-octylthiophene) (P3OT) are used for this purpose. These blends are then spin coated onto a transparent conductive electrode with thicknesses that vary from 60 to 120 nm. These conductive electrodes are usually glass covered with indium tin oxide (ITO) and a 40 nm sublayer of poly(3,4-ethylenedioxythiophene) (PEDOT) and poly(styrenesulfonate) (PSS). PEDOT and PSS help to smooth the ITO surface, decreasing the density of pinholes and stifling current leakage that occurs along shunting paths. Through thermal evaporation or sputter coating, a 20 to 70 nm thick layer of aluminum and sometimes an intermediate layer of lithium fluoride are then applied onto the photoactive material. Multiple research investigations with both multi-walled carbon nanotubes (MWCNTs) and single-walled carbon nanotubes (SWCNTs) integrated into the photoactive material have been completed.[3][1][2][4][5][6][7]
Enhancements of more than two orders of magnitude have been observed in the photocurrent from adding SWCNTs to the P3OT matrix.[2] Improvements were speculated to be due to charge separation at polymer–SWCNT connections and more efficient electron transport through the SWCNTs. However, a rather low power conversion efficiency of 0.04% under 100 mW/cm2 white illumination was observed for the device suggesting incomplete exciton dissociation at low CNT concentrations of 1.0% wt. Because the lengths of the SWCNTs were similar to the thickness of photovoltaic films, doping a higher percentage of SWCNTs into the polymer matrix was believed to cause short circuits. To supply additional dissociation sites, other researchers have physically blended functionalized MWCNTs into P3HT polymer to create a P3HT-MWCNT with fullerene C60 double-layered device.[8] However, the power efficiency was still relatively low at 0.01% under 100 mW/cm2 white illumination. Weak exciton diffusion toward the donor–acceptor interface in the bilayer structure may have been the cause in addition to the fullerene C60 layer possibly experiencing poor electron transport.
More recently, a polymer photovoltaic device from C60-modified SWCNTs and P3HT has been fabricated.[9] Microwave irradiating a mixture of aqueous SWCNT solution and C60 solution in toluene was the first step in making these polymer-SWCNT composites. Conjugated polymer P3HT was then added resulting in a power conversion efficiency of 0.57% under simulated solar irradiation (95 mW/cm2). It was concluded that improved short circuit current density was a direct result of the addition of SWCNTs into the composite causing faster electron transport via the network of SWCNTs. It was also concluded that the morphology change led to an improved the fill factor. Overall, the main result was improved power conversion efficiency with the addition of SWCNTs, compared to cells without SWCNTs; however, further optimization was thought to be possible.
Additionally, it has been found that heating to the point beyond the glass transition temperature of either P3HT or P3OT after construction can be beneficial for manipulating the phase separation of the blend. This heating also affects the ordering of the polymeric chains because the polymers are microcrystalline systems and it improves charge transfer, charge transport, and charge collection throughout the OPV device. The hole mobility and power efficiency of the polymer-CNT device also increased significantly as a result of this ordering.[10]
Emerging as another valuable approach for deposition, the use of tetraoctylammonium bromide in tetrahydrofuran has also been the subject of investigation to assist in suspension by exposing SWCNTs to an electrophoretic field.[11] In fact, photoconversion efficiencies of 1.5% and 1.3% were achieved when SWCNTs were deposited in combination with light harvesting cadmium sulfide (CdS) quantum dots and porphyrins, respectively.[12]
Among the best power conversions achieved to date using CNTs were obtained by depositing a SWCNT layer between the ITO and the PEDOT : PSS or between the PEDOT : PSS and the photoactive blend in a modified ITO/PEDOT : PSS/ P3HT : (6,6)-phenyl-C61-butyric acid methyl ester (PCBM)/Al solar cell. By dip-coating from a hydrophilic suspension, SWCNT were deposited after an initially exposing the surface to an argon plasma to achieve a power conversion efficiency of 4.9%, compared to 4% without CNTs.[13]
However, even though CNTs have shown potential in the photoactive layer, they have not resulted in a solar cell with a power conversion efficiency greater than the best tandem organic cells (6.5% efficiency).[14] But, it has been shown in most of the previous investigations that the control over a uniform blending of the electron donating conjugated polymer and the electron accepting CNT is one of the most difficult as well as crucial aspects in creating efficient photocurrent collection in CNT-based OPV devices. Therefore, using CNTs in the photoactive layer of OPV devices is still in the initial research stages and there is still room for novel methods to better take advantage of the beneficial properties of CNTs.

Carbon nanotubes as a transparent electrode

ITO is currently the most popular material used for the transparent electrodes in OPV devices; however, it has a number of deficiencies. For one, it is not very compatible with polymeric substrates due to its high deposition temperature of around 600o C. Traditional ITO also has unfavorable mechanical properties such as being relatively fragile. In addition, the combination of costly layer deposition in vacuum and a limited supply of indium results in high quality ITO transparent electrodes being very expensive. Therefore, developing and commercializing a replacement for ITO is a major focus of OPV research and development.
Conductive CNT coatings have recently become a prospective substitute based on wide range of methods including spraying, spin coating, casting, layer-by-layer, and Langmuir–Blodgett deposition.[3][15][16][17] The transfer from a filter membrane to the transparent support using a solvent or in the form of an adhesive film is another method for attaining flexible and optically transparent CNT films.[18] Other research efforts have shown that films made of arc-discharge CNT can result in a high conductivity and transparency.[19] Furthermore, the work function of SWCNT networks is in the 4.8 to 4.9 eV range (compared to ITO which has a lower work function of 4.7 eV) leading to the expectation that the SWCNT work function should be high enough to assure efficient hole collection.[20] Another benefit is that SWCNT films exhibit a high optical transparency in a broad spectral range from the UV-visible to the near-infrared range. Only a few materials retain reasonable transparency in the infrared spectrum while maintaining transparency in the visible part of the spectrum as well as acceptable overall electrical conductivity.[18] SWCNT films are highly flexible, do not creep, do not crack after bending, theoretically have high thermal conductivities to tolerate heat dissipation, and have high radiation resistance. However, the electrical sheet resistance of ITO is an order of magnitude less than the sheet resistance measured for SWCNT films. Nonetheless, initial research studies demonstrate SWCNT thin films can be used as conducting, transparent electrodes for hole collection in OPV devices with efficiencies between 1% and 2.5% confirming that they are comparable to devices fabricated using ITO.[20][21] Thus, possibilities exist for advancing this research to develop CNT-based transparent electrodes that exceed the performance of traditional ITO materials.

CNTs in dye-sensitized solar cells

Due to the simple fabrication process, low production cost, and high efficiency, there is significant interest in dye-sensitized solar cells (DSSCs). Thus, improving DSSC efficiency has been the subject of a variety of research investigations because it has the potential to be manufactured economically enough to compete with other solar cell technologies. Titanium dioxide nanoparticles have been widely used as a working electrode for DSSCs because they provide a high efficiency, more than any other metal oxide semiconductor investigated.[22] Yet the highest conversion efficiency under air mass (AM) 1.5 (100 mW/cm2) irradiation reported for this device to date is about 11%.[23] Despite this initial success, the effort to further enhance efficiency has not produced any major results.[24] The transport of electrons across the particle network has been a key problem in achieving higher photoconversion efficiency in nanostructured electrodes. Because electrons encounter many grain boundaries during the transit and experience a random path, the probability of their recombination with oxidized sensitizer is increased.[25] Therefore, it is not adequate to enlarge the oxide electrode surface area to increase efficiency because photo-generated charge recombination should be prevented. Promoting electron transfer through film electrodes and blocking interface states lying below the edge of the conduction band are some of the non-CNT based strategies to enhance efficiency that have been employed.[24]
With recent progress in CNT development and fabrication, there is promise to use various CNT based nanocomposites and nanostructures to direct the flow of photogenerated electrons and assist in charge injection and extraction. To assist the electron transport to the collecting electrode surface in a DSSC, a popular concept is to utilize CNT networks as support to anchor light harvesting semiconductor particles. Research efforts along these lines include organizing CdS quantum dots on SWCNTs.[12] Charge injection from excited CdS into SWCNTs was documented upon excitation of CdS nanoparticles. Other varieties of semiconductor particles including CdSe and CdTe can induce charge-transfer processes under visible light irradiation when attached to CNTs.[26] Including porphyrin and C60 fullerene, organization of photoactive donor polymer and acceptor fullerene on electrode surfaces has also been shown to offer considerable improvement in the photoconversion efficiency of solar cells.[27] Therefore, there is an opportunity to facilitate electron transport and increase the photoconversion efficiency of DSSCs utilizing the electron-accepting ability of semiconducting SWCNTs.
Other researchers fabricated DSSCs using the sol-gel method to obtain titanium dioxide coated MWCNTs for use as an electrode.[24] Because pristine MWCNTs have a hydrophobic surface and poor dispersion stability, pretreatment was necessary for this application. A relatively low-destruction method for removing impurities, H2O2 treatment was used to generate carboxylic acid groups by oxidation of MWCNTs. Another positive aspect was the fact that the reaction gases including CO2 and H2O were non-toxic and could be released safely during the oxidation process. As a result of treatment, H2O2 exposed MWCNTs have a hydrophilic surface and the carboxylic acid groups on the surface have polar covalent bonding. Also, the negatively charged surface of the MWCNTs improved the stability of dispersion. By then entirely surrounding the MWCNTs with titanium dioxide nanoparticles using the sol-gel method, an increase in the conversion efficiency of about 50% compared to a conventional titanium dioxide cell was achieved. The enhanced interconnectivity between the titanium dioxide particles and the MWCNTs in the porous titanium dioxide film was concluded to be the cause of the improvement in short circuit current density. Here again, the addition of MWCNTs was thought to provide more efficient electron transfer through film in the DSSC.

Thermal properties of nanostructures


General considerations

As the devices continue to shrink further into the sub-100 nm range following the trend predicted by Moore’s law, the topic of thermal properties and transport in such nanoscale devices becomes increasingly important. Display of great potential by nanostructures for thermoelectric applications also motivates the studies of thermal transport in such devices.[1] These fields, however, generate two contradictory demands: high thermal conductivity to deal with heating issues in sub-100 nm devices and low thermal conductivity for thermoelectric applications. These issues can be addressed with phonon engineering, once nanoscale thermal behaviors have been studied and understood.[2]

The effect of the limited length of structure

In general two carrier types can contribute to thermal conductivity - electrons and phonons. In nanostructures phonons usually dominate and the phonon properties of the structure become of a particular importance for thermal conductivity.[1][3][4] These phonon properties include: phonon group velocity, phonon scattering mechanisms, heat capacity, Grüneisen parameter. Unlike bulk materials, nanoscale devices have thermal properties which are complicated by boundary effects due to small size. It has been shown that in some cases phonon-boundary scattering effects dominate the thermal conduction processes, reducing thermal conductivity.[1][5]
Depending on the nanostructure size, the phonon mean free path values (Λ) may be comparable or larger than the object size. When L is larger than the phonon mean free path, Umklapp scattering process limits thermal conductivity (regime of diffusive thermal conductivity). When L is comparable to or smaller than the mean free path (which is of the order 1 µm for carbon nanostructures[6]), the continuous energy model used for bulk materials no longer applies and nonlocal and nonequilibrium aspects to heat transfer also need to be considered.[1] In this case phonons in defectless structure could propagate without scattering and thermal conductivity becomes ballistic (similar to ballistic conductivity). More severe changes in thermal behavior are observed when the feature size L shrinks further down to the wavelength of phonons.[7]

Features of different nanostructures

In the following section, we will detail the thermal properties of common nanostructures including nanowires, nanotubes, and thin films.

Nanowires

Thermal conductivity measurements

The first measurement of thermal conductivity in silicon nanowires was published in 2003.[5] Two important features were pointed out: 1) The measured thermal conductivities are significantly lower than that of the bulk Si and, as the wire diameter is decreased, the corresponding thermal conductivity is reduced. 2) As the wire diameter is reduced, the phonon boundary scattering dominates over phonon–phonon Umklapp scattering, which decreases the thermal conductivity with an increase in temperature.
For 56 nm and 115 nm wires k ~ T3 dependence was observed, while for 37 nm wire k ~ T2 dependence and for 22 nm wire k ~ T dependence were observed. Chen et al. [8] has shown that the one-dimensional cross-over for 20 nm Si nanowire occurs around 8K, while the phenomenon was observed for temperature values greater than 20K. Therefore the reason of such behaviour is not in the confinement experienced by phonons so that three-dimensional structures display two-dimensional or one-dimensional behavior.

Theoretical models for nanowires

Different phonon modes contribution to thermal conductivity
Assuming that Boltzmann transport equation is valid, thermal conductivity can be written as:
k=\frac{1}{3}Cv_g\Lambda=\frac{1}{3}Cv_g^2\tau
where C is the heat capacity, vg is the group velocity and τ is the relaxation time. Note that this assumption breaks down when the dimensions of the system are comparable to or smaller than the wavelength of the phonons responsible for thermal transport. In our case, phonon wavelengths are generally in the 1 nm range [9] and the nanowires under consideration are within tens of nanometers range, the assumption is valid.
Different phonon mode contributions to heat conduction can be extracted from analysis of the experimental data for silicon nanowires of different diameters [1] to extract the C·vg product for analysis. It was shown that all phonon modes contributing to thermal transport are excited well below the Si Debye temperature (645 K).
From the thermal conductivity equation, one can write the product C·vg for each isotropic phonon branch i.
(Cv_g)_i=\frac{k_B^4 T^3}{2\hbar^3\pi^2}\int \frac{1}{v_{p,i}^2}\left[\frac{x^4 exp(x)}{(exp(x)-1)^2}\right]\,dx
where x = hω / kBT and vp,i is the phonon phase velocity, which is less sensitive to phonon dispersions than the group velocity vg.
Many models of phonon thermal transport ignores the effects of transverse acoustic phonons (TA) at high frequency due to their small group velocity. (Optical phonon contributions are also ignored for the same reason.) However, upper branch of TA phonons have non-zero group velocity at the Brillouin zone boundary along the Γ-Κ direction and, in fact, behave similarly to the longitudinal acoustic phonons (LA) and can contribute to the heat transport.
Then, the possible phonon modes contributing to heat conduction are both LA and TA phonons at low and high frequencies. Using the corresponding dispersion curves, the C·vg product can then be calculated and fitted to the experimental data. The best fit was found when contribution of high-frequency TA phonons is accounted as 70% of the product at room temperature. The remaining 30% is contributed by the LA and TA phonons at low-frequency.
 Using complete phonon dispersions
Thermal conductivity in nanowires can be computed based on complete phonon dispersions instead of the linearlized dispersion relations commonly used to calculate thermal conductivity in bulk materials.[10]
Assuming the phonon transport is diffusive and Boltzmann transport equation (BTE) is valid, nanowire thermal conductance G(T) can be defined as:
 G(T) \simeq \sum_{\alpha}{\int{ \frac{\lambda_a(k_z)}{L} \frac{\hbar \omega_{\alpha}(k_z)}{2\pi} \frac{df_b}{dT}v_z(\alpha,k_z)dk_z}}
where the variable α represents discrete quantum numbers associated with sub-bands found in one-dimensional phonon dispersion relations, fB represents the Bose-Einstein distribution, vz is the phonon velocity in the z direction and λ is the phonon relaxation length along the direction of the wire length. Thermal conductivity is then expressed as:
k(T)=\frac{1}{S} \sum{\alpha} {\int_{0}^{\frac{\pi}{a_z}} \lambda_\alpha (k_z) \frac{\hbar\omega_\alpha (k_z)}{2\pi}\frac{df_B}{dT}v_z(\alpha,k_z)\, dk_z}
where S is the cross sectional area of the wire, az is the lattice constant.
It was shown [10] that, using this formula and atomistically computed phonon dispersions (with interatomic potentials developed in [11]), it is possible to predictively calculate lattice thermal conductivity curves for nanowires, in good agreement with experiments. On the other hand, it was not possible to obtain correct results with the approximated Callaway formula.[12] These results are expected to apply to ”nanowhiskers” for which phonon confinement effects are unimportant. Si nanowires wider than ~35 nm are within this category.[10]
Very thin nanowires
For large diameter nanowires, theoretical models assuming the nanowire diameters are comparable to the mean free path and that the mean free path is independent of phonon frequency have been able to closely match the experimental results. But for very thin nanowires whose dimensions are comparable to the dominant phonon wavelength, a new model is required. The study in [8] has shown that in such cases, the phonon-boundary scattering is dependent on frequency. The new mean free path is then should be used:
 l^{-1} = B \left(\frac{h}{d}\right)^2 \frac{1}{d} \left(\frac{\omega}{\omega_D}\right)^2N(\omega)
Here, l is the mean free path (same as Λ). The parameter h is length scale associated with the disordered region, d is the diameter, N(ω) is number of modes at frequency ω, and B is a constant related to the disorder region.[8]
Thermal conductance is then calculated using Landauer formula:
 G(T) = \frac{1}{2 \pi \hbar} \int_0^{\infty}{ \left(\frac{N_1(\omega)}{1+L/l(\omega)}+\frac{N_2(\omega)}{1+L/d}\right)\frac{\hbar^3 \omega^2}{k_B T^2} \times \frac{e^{\frac{\hbar \omega}{k_B T}}}{{(e^\frac{\hbar\omega}{k_BT}-1)}^2} }

Carbon nanotubes

As nanoscale graphitic structures, carbon nanotubes are of great interest for their thermal properties. The low-temperature specific heat and thermal conductivity show direct evidence of 1-D quantization of the phonon band structure. Modeling of the low-temperature specific heat allows determination of the on-tube phonon velocity, the splitting of phonon subbands on a single tube, and the interaction between neighboring tubes in a bundle.

Thermal conductivity measurements

Measurements show a single-wall carbon nanotubes (SWNTs) room-temperature thermal conductivity about 3500 W/(m·K),[13] and over 3000 W/(m·K) for individual multiwalled carbon nanotubes (MWNTs).[14] Addition of nanotubes to epoxy resin can double the thermal conductivity for a loading of only 1%, showing that nanotube composite materials may be useful for thermal management applications.

Theoretical models for nanotubes

Thermal conductivity in CNT is mainly due to phonons rather than electrons [3] so the Wiedemann–Franz law is not applicable.
In general, the thermal conductivity is a tensor quality, but for this discussion, it is only important to consider the diagonal elements:
k_{zz} = \sum C{v_z}^2\tau
where C is the specific heat, and vz and τ are the group velocity and relaxation time of a given phonon state.
At low temperatures (T is far less than Debye temperature), the relaxation time is determined by scattering of fixed impurities, defects, sample boundaries, etc. and is roughly constant. Therefore, in ordinary materials, the low-temperature thermal conductivity has the same temperature dependence as the specific heat. However, in anisotropic materials, this relationship does not strictly hold. Because the contribution of each state is weighted by the scattering time and the square of the velocity, the thermal conductivity preferentially samples states with large velocity and scattering time. For instance, in graphite, the thermal conductivity parallel to the basal planes is only weakly dependent on the interlayer phonons. In SWNT bundles, it is likely that k(T) depends only on the on-tube phonons, rather than the intertube modes.
Thermal conductivity is of particular interest in low-dimensional systems. For CNT, represented as 1-D ballistic electronic channel, the electronic conductance is quantized, with a universal value of
G_0 = \frac{2e^2}{h}
Similarly, for a single ballistic 1-D channel, the thermal conductance is independent of materials parameters, and there exists a quantum of thermal conductance, which is linear in temperature [15]:
G_{th} = \frac{\pi^2 {k_B}^2 T}{3h}
Possible conditions for observation of this quantum were examined by Rego and Kirczenow.[16] In 1999, Keith Schwab, Erik Henriksen, John Worlock, and Michael Roukes carried out a series of experimental measurements that enabled first observation of the thermal conductance quantum.[17] The measurements employed suspended nanostructures coupled to sensitive dc SQUID measurement devices. In 2008, a colorized electron micrograph of one of the Caltech devices was acquired for the permanent collection of the Museum of Modern Art in New York.
At high temperatures, three-phonon Umklapp scattering begins to limit the phonon relaxation time. Therefore the phonon thermal conductivity displays a peak and decreases with increasing temperature. Umklapp scattering requires production of a phonon beyond the Brillouin zone boundary; because of the high Debye temperature of diamond and graphite, the peak in the thermal conductivity of these materials is near 100 K, significantly higher than for most other materials. In less crystalline forms of graphite, such as carbon fibers, the peak in k(T) occurs at higher temperatures, because defect scattering remains dominant over Umklapp scattering to higher temperature.[18] In low-dimensional systems, it is difficult to conserve both energy and momentum for Umklapp processes,[19] and so it may be possible that Umklapp scattering is suppressed in nanotubes relative to 2-D or 3-D forms of carbon.
Berber et al.[20] have calculated the phonon thermal conductivity of isolated nanotubes. The value k(T) peaks near 100 K, and then decreases with increasing temperature. The value of k(T) at the peak (37,000 W/(m·K)) is comparable to the highest thermal conductivity ever measured (41,000 W/(m·K) for an isotopically pure diamond sample at 104 K). Even at room temperature, the thermal conductivity is quite high (6600 W/(m·K)), exceeding the reported room-temperature thermal conductivity of isotopically pure diamond by almost a factor of 2.
In graphite, the interlayer interactions quench the thermal conductivity by nearly 1 order of magnitude[citation needed]. It is likely that the same process occurs in nanotube bundles[citation needed]. Thus it is significant that the coupling between tubes in bundles is weaker than expected[citation needed]. It may be that this weak coupling, which is problematic for mechanical applications of nanotubes, is an advantage for thermal applications.
Phonon density of states for nanotubes
The phonon density of states is to calculated through band structure of isolated nanotubes, which is studied in Saito et al.[21][22] and Sanchez-Portal et al.[23] When a graphene sheet is ‘‘rolled’’ into a nanotube, the 2-D band structure folds into a large number of 1-D subbands. In a (10,10) tube, for instance, the six phonon bands (three acoustic and three optical) of the graphene sheet become 66 separate 1-D subbands. A direct result of this folding is that the nanotube density of states has a number of sharp peaks due to 1-D van Hove singularities, which are absent in graphene and graphite. Despite the presence of these singularities, the overall density of states is similar at high energies, so that the high temperature specific heat should be roughly equal as well. This is to be expected: the high-energy phonons are more reflective of carbon–carbon bonding than the geometry of the graphene sheet.

Thin films

Thin films are prevalent in the micro and nanoelectronics industry for the fabrication of sensors, actuators and transistors; thus, thermal transport properties affect the performance and reliability of many structures such as transistors, solid-state lasers, sensors, and actuators. Although these devices are traditionally made from bulk crystalline material (silicon), they often contain thin films of oxides, polysilicon, metal, as well as superlattices such as thin-film stacks of GaAs/AlGaAs for lasers.

Single-crystal thin films

Silicon-on-insulator (SOI) films with silicon thicknesses of 0.05 µm to 10 µm above a buried silicon dioxide layer are increasingly popular for semiconductor devices due to the increased dielectric isolation associated with SOI/[24] SOI wafers contain a thin-layer of silicon on an oxide layer and a thin-film of single-crystal silicon, which reduces the effective thermal conductivity of the material by up to 50% as compared to bulk silicon, due to phonon-interface scattering and defects and dislocations in the crystalline structure. It was suggestedthat there is a weak dependence on film thickness, provided that thermal conductivity is mainly limited by dislocations in the membrane structure rather than phonon-boundary scattering effects.[25] Previous studies by Asheghi et al., show a similar trend.[24] Other studies of thin-films show similar thermal effects[citation needed].

Superlattices

Thermal properties associated with superlattices are critical in the development of semiconductor lasers. Heat conduction of superlattices is less understood than homogeneous thin films. It is theorized that superlattices have a lower thermal conductivity due to impurities from lattice mismatches and at the heterojunctions. Phonon-interface scattering at heterojunctions needs to be considered in this case; fully elastic scattering underestimates the heat conduction, while fully inelastic scattering overestimates the heat conduction.[26][27] For example, a Si/Ge thin-film superlattice has a greater decrease in thermal conductivity than an AlAs/GaAs film stack [28] due to increased lattice mismatch. A simple estimate of heat conduction of superlattices is:
 k_n = \left( \frac{C_1 v_1 C_2 v_2}{C_1 v_1 + C_2 v_2} \right) \left( \frac{d_1 + d_2}{2} \right)
where C1 and C2 are the corresponding heat capacity of film1 and film2 respectively, v1 and v2 are the acoustic propagation velocities in film1 and film2, and d1 and d2 are the thicknesses of film1 and film2. This model neglects scattering within the layers and assumes fully diffuse, inelastic scattering.[29]

Polycrystalline films

Polycrystalline films are common in semiconductor devices, as the gate electrode of a field-effect transistor is often made of polycrystalline silicon. If the polysilicon grain sizes are small, internal scattering from grain boundaries can overwhelm the effects of film-boundary scattering. Also, grain boundaries contain more impurities, which result in impurity scattering. Likewise, disordered or amorphous films will experience a severe reduction of thermal conductivity, since the small grain size results in numerous grain-boundary scattering effects.[30] Different deposition methods of amorphous films will result in differences in impurities and grain sizes.[29]
The simplest approach to modeling phonon scattering at grain boundaries is to increase the scattering rate by introducing this equation:
\tau_G^{-1}=B\frac{v}{d_G}
where B is a dimensionless parameter that correlates with the phonon reflection coefficient at the grain boundaries, dG is the characteristic grain size, and v is the phonon velocity through the material. A more formal approach to estimating the scattering rate is:
 {\tau_G}^{-1} = \frac{2 \nu}{\pi d_G} \left[ 1-exp\left(-\frac{\pi^2}{4}\nu_G \right) \right]
where vG is the dimensionless grain-boundary scattering strength, defined as
νG = ∑ σjνj

j
Here σj is the cross-section of a grain-boundary area, and νj is the density of the grain boundary area.[29]

Measuring thermal conductivity of thin films

There are two approaches to experimentally determine the thermal conductivity of thin films. The goal of experimental metrology of thermal conductivity of thin films is to attain an accurate thermal measurement without disturbing the properties of the thin-film.
Electrical heating is used for thin films which have a lower thermal conductivity than the substrate; it is fairly accurate in measuring out-of-plane conductivity. Often, a resistive heater and thermistor is fabricated on the sample film using a highly conductive metal, such as aluminium. The most straightforward approach would be to apply a steady-state current and measure the change in temperature of adjacent thermistors. A more versatile approach uses an AC signal applied to the electrodes. The third harmonic of the AC signal reveals heating and temperature fluctuations of the material.[29]
Laser heating is a non-contact metrology method, which uses picosecond and nanosecond laser pulses to deliver thermal energy to the substrate. Laser heating uses a pump-probe mechanism; the pump beam introduces energy to the thin-film, as the probe beam picks up the characteristics of how the energy propagates through the film. Laser heating is advantageous because the energy delivered to the film can be precisely controlled; furthermore, the short heating duration decouples the thermal conductivity of the thin film from the substrate[citation needed].

Carbon nanotube spring

Carbon nanotube springs are springs made of carbon nanotubes (CNTs). They are an alternate form of high density, lightweight, reversible energy storage based on the elastic deformations of CNTs. Many previous studies on the mechanical properties of CNTs have revealed that they possess high stiffness, strength and flexibility. The Young's modulus of CNTs is 1TPa and they have the ability to sustain reversible tensile strains of 6%[1] and the mechanical springs based on these structures are likely to surpass the current energy storage capabilities of existing steel springs and provide a viable alternative to electrochemical batteries. The obtainable energy density is predicted to be highest under tensile loading, with an energy density in the springs themselves about 2500 times greater than the energy density that can be reached in steel springs, and 10 times greater than the energy density of lithium-ion batteries.
The process of elastic energy storage in a CNT involves in deforming it under an applied load. On removal of the applied load the energy released from the CNT can be used to perform mechanical work. A CNT has the ability to deform reversibly and a spring made from it can undergo repeated charge-discharge cycles without fatigue.
A CNT spring can store elastic strain energy with a density several orders of magnitude higher than conventional springs made of steel. Strain energy density in a material is proportional to the product of its Young's modulus and the square of the applied strain.
When multi-walled nanotubes (MWCNTs) are loaded, the majority of the applied load is borne by the outer shell. It is due to this limited load transfer between the different layers of MWCNTs that single walled nanotubes (SWCNTs) are more useful structural materials for springs

Energy storage in CNT springs

Springs for energy storage can be made of SWCNTs or MWCNTs arranged in dense bundles of long, aligned tubes called 'forests' of CNTs [2] that are grown by chemical vapor deposition(CVD). The 'forests' can grow to heights of up to 6mm.[3]. A deformed CNT requires a support structure to carry the load of the spring prior to discharge. A mechanical spring must be coupled to external mechanisms to build a power source that is functionally useful. On its own a spring stores potential energy when an external force is applied to it but releases the energy in a single rapid burst once the force is removed. An effective power source needs to store energy over a period of time, release the energy only when needed and discharge the energy at a desired power level. A CNT based portable power source should have a basic architecture made of four main components: a CNT spring, a supporting structure for the spring, a generator-motor combination, and a coupling mechanism between the spring and the generator.
For CNTs arranged in groups/bundles called 'forests' as described earlier, efficient packing and good alignment in necessary between the tubes to achieve a high energy density. Good load transfer and effective attachment techniques are required so that the shells can be loaded to near their elastic limit.
Choosing the appropriate deformation mode consisting of any amongst axial tension, axial compression, torsion or bending or a combination of any of them. A criteria for choosing a deformation mode is not only the highest energy density but also the proper integration of the deformed spring with the rest of the power dissipation mechanism.
A support structure is required to hold the CNT spring in the fully loaded configuration prior to its release . The design of the support structure will depend on the scale of the spring, the deformation mode the CNT is being subjected to and the architecture of the rest of the system. The material selected for the structure should have high strength because the added mass and volume of the support contribute to reducing the energy density of the entire system.

Energy storage calculations

Axial tension

Analysis is performed on CNTs subject to tensile loads. A hollow cylindrical structure of CNT of length L, diameter d and mean radius r is considered. The tube has thickness n.h, where n is the number of layers in the CNT and h=0.34 nm is the thickness of one shell. The Young's modulus of the material of the CNT is E. In case of SWCNTs, n=1 and n>1 in case of MWCNTs. The cylinder has inner and outer radii of
 r_i = r - \frac{nh}{2}
and
 r_o = r + \frac{nh}{2}.
The shell's cross-sectional area is
 A = \pi(r_o^2 - r_i^2)
and the total enclosed area is
 A_t = \pi r_o^2 .
The strain energy that can be stored in the bar under axial compression to a strain of \epsilon\, is
U =\frac{1}{2} \iiint (\sigma_x\,\epsilon_x\,)\, dx\, dy\, dz =\frac{1}{2}E\epsilon^2\ AL = \frac{1}{2}E\epsilon^2\pi (r_o^2 - r_i^2) L
The strain energy density is simply the ratio of the strain energy and the enclosed volume. Therefore in order for the strain energy density to be high the value of A / At should be large. So, a spring in axial tension should consist of either SWCNTs with small diameters or uniformly loaded MWCNTs with densely packed shells to maximize A / At.
The CNTs are arranged in groupings, generally bundles. The strain energy density must be reduced by a fill factor k to account for the spacing between the individual CNTs.
Consider the cross-section of a bundle of closely packed SWCNTs of radius r, arranged into a two-dimensional triangular lattice with a lattice constant of 2r+h. Ideal packing is assumed with a spacing of h=0.34 nm which is taken equal to the graphitic spacing. When the CNTs are arranged in a bundle the best packing fraction is produced when they are packed in a hexagonal closed packed structure.
Consider a cross section of one bundle. A hexagonal shape will be observed. The hexagonal shape with an area of Ah is taken to be the repeating geometrical unit in the bundle. Calculations can be performed to show that fill factor k =91%. In reality, there may not be ideal packing within a bundle, as the actual fraction k may be lower than the value calculated.
The expression of strain energy shows that it is advantageous to apply a high tensile strain to the springs to maximize energy storage since strain energy is proportional to square of the strain.

Axial compression

Analysis is performed on CNTs subject to compressive loads. The CNT is assumed to be a hollow cylindrical beam of length L, Young's modulus E, and thickness n.h, where n is the number of layers and h=0.34 nm is the thickness of one shell(taken equal to the separation between graphene sheets in graphite). The continuous tube has a mean radius r and diameter d. The cylinder has inner and outer radii of
 r_i = r - \frac{nh}{2}
and
 r_o = r + \frac{nh}{2}.
The shell's cross-sectional area is
 A = \pi(r_o^2 - r_i^2)
and the total enclosed area is
 A_t = \pi r_o^2 .
The strain energy that can be stored in the bar under axial compression to a strain of \epsilon\, is
U =\frac{1}{2} \iiint (\sigma_x\,\epsilon_x\,)\, dx\, dy\, dz =\frac{1}{2}E\epsilon^2\ AL = \frac{1}{2}E\epsilon^2\pi (r_o^2 - r_i^2) L
The strain energy density is just the strain energy divided by the enclosed volume. High energy densities are achieved with a high A / At ratio. Therefore in order for CNT springs to achieve a high energy density either SWCNTs with small diameters or MWCNTs with densely packed shells should be used.

The Support structure

The purpose of using a support structure is to be able to store energy before it is released for use. The support structure should be strong enough to support the applied load (used to compress the CNTs) without reaching failure itself. Another point of consideration is that the energy density of the combined spring and supporting structure is always lower than the energy density of the spring alone.

Energy density comparison

A CNT spring made of bundles of densely packed 1 nm diameter SWCNTs stretched to a 10% strain is predicted to have an energy density of 3.4x106kJ/m3[4]. The energy density of CNT springs loaded in tension is higher than the energy density of CNT springs loaded in compression[5]. Whereas the current maaximum energy density of a carbon-steel watch spring is reported to be between 1080kJ/m3[6] and 3000kJ/m3[7]. Calculations show that when a support structure made of single crystal silicon carbide is used the energy density of CNT springs reduces to 1x106kJ/m3. Even after considering a support structure and other energy extraction hardware associated with a CNT spring energy harvesting device, its energy density is much greater than mechanical springs and is in approximately the same range as that of lithium-ion batteries. The energy density is much lower than the energy density of any hydrocarbon used in combustion processes.

Failure processes that limit energy storage

A large number of CNTs are needed to store a significant amount of energy that can be used for macroscopic processes.And in order to achieve such large amount of energy storage the CNT springs must maintain high stiffness and elasticity. It is practically quite difficult to have such high stiffness and elastic strains in yarns or fibers made up of assemblies of CNTs as they seldom maintain mechanical properties of an individual SWCNT. This behavior occurs due to atomic defects and imperfect organisation.
Elastic loading is the preferred loading mechanism for reversible energy storage, experiments have been performed that indicate that loading within the fibers deviates from purely elastic behavior.
Only a portion of the CNTs contribute to the load bearing at a given strain. The unequal amount of slack within each CNT due to the presence of atomic defects and tangling causes different CNTs to fracture at different strains.
When CNTs are loaded in tension it is difficult to grasp the inner shells in case of MWCNTs. Tensile tests of MWCNTs attached to atomic force microscope (AFM) tips at both ends show that fracture occurs at the outer shell in a way such that majority loading occurs at the outer shell and little load transfer occurs to the inner shells. This causes the stiffness and strength of MWCNTs to be lower than the case when the shells would be loaded equally.

Carbon nanotube field-effect transistor


A carbon nanotube field-effect transistor (CNTFET) refers to a field-effect transistor that utilizes a single carbon nanotube or an array of carbon nanotubes as the channel material instead of bulk silicon in the traditional MOSFET structure. Since it was first demonstrated in 1998, there have been tremendous developments in CNTFETs, which promise for an alternative material to replace silicon in future electronics.[1]

Introduction and background

A schematic animations of a carbon nanotube that can be formed by rolling up graphene
 
According to Moore's law, the dimensions of individual devices in an integrated circuit have been decreased by a factor of approximately two every two years. This scaling down of devices has been the driving force in technological advances since late 20th century. However, as noted by ITRS 2009 edition, further scaling down has faced serious limits related to fabrication technology and device performances as the critical dimension shrunk down to sub-22 nm range.[2] The limits involve electron tunneling through short channels and thin insulator films, the associated leakage currents, passive power dissipation, short channel effects, and variations in device structure and doping.[3] These limits can be overcome to some extent and facilitate further scaling down of device dimensions by modifying the channel material in the traditional bulk MOSFET structure with a single carbon nanotube or an array of carbon nanotubes.

Electronic structure of carbon nanotubes

Graphene atomic structure with a translational vector T and a chiral vector Ĉh of a CNT
One-dimensional energy dispersion relations for (a) (n,m)=(5,5) metallic tube, (b) (n,m)=(10,0) semiconducting tube.
The exceptional electrical properties of carbon nanotubes arise from the unique electronic structure of graphene itself that can roll up and form a hollow cylinder. The circumference of such carbon nanotube can be expressed in terms of a chiral vector: Ĉh=nâ1+mâ2 which connects two crystallographically equivalent sites of the two-dimensional graphene sheet. Here n and m are integers and â1 and â2 are the unit vectors of the hexagonal honeycomb lattice. Therefore, the structure of any carbon nanotube can be described by an index with a pair of integers (n,m) that define its chiral vector.
In terms of the integers (n,m), the nanotube diameter dt is given by: Diameter and the chiral angle θ is given by:
 \theta = \tan^{-1}\left(\frac{\sqrt{3}\,n}{2m+n}\right) .[4]
The differences in the chiral angle and the diameter cause the differences in the properties of the various carbon nanotubes. For example, it can be shown that an (n,m) carbon nanotube is metallic when n = m, has a small gap when n – m = 3i, where i is an integer, and is semiconducting when n – m ≠ 3i.[5] This is due to the fact that the periodic boundary conditions for the one-dimensinal carbon nanotubes permit only a few wave vectors to exist around the circumference of carbon nanotubes. Metallic conduction occurs when one of these wave vectors passes through the K-point of graphene’s 2D hexagonal Brillouin zone, where the valence and conduction bands are degenerate.[4] For the semiconducting carbon nanotubes, there is a diameter dependency on bangap. For example, according to a single-particle tight-binding description of the electronic structure, Cntbandgap where γ is the hopping matrix element, and a is the carbon-carbon bond distance.[6]

Motivations for transistor applications

A carbon nanotube’s bandgap is directly affected by its chirality and diameter. If those properties can be controlled, CNTs would be a promising candidate for future nano-scale transistor devices. Moreover, because of the lack of boundaries in the perfect and hollow cylinder structure of CNTs, there is no boundary scattering. CNTs are also quasi-1D materials in which only forward scattering and back scattering are allowed, and elastic scattering mean free paths in carbon nanotubes are long, typically on the order of micrometers. As a result, quasi-ballistic transport can be observed in nanotubes at relatively long lengths and low fields.[7] Because of the strong covalent carbon-carbon bonding in the sp2 configuration, carbon nanotubes are chemically inert and are able to transport large amounts of electric current. In theory, carbon nanotubes are also able to conduct heat nearly as well as diamond or sapphire, and because of their miniaturized dimensions, the CNTFET should switch reliably using much less power than a silicon-based device.[8]

Device fabrication

There are many types of CNTFET devices; a general survey of the most common geometries are covered below.

Back-gated CNTFETs

Top view
Top view
Side view
Side view
Top and side view of carbon nanotubes deposited on a silicon oxide substrate pre-patterned with source and drain contacts.
The earliest techniques for fabricating carbon nanotube (CNT) field-effect transistors involved pre-patterning parallel strips of metal across a silicon dioxide substrate, and then depositing the CNTs on top in a random pattern.[1][9] The semiconducting CNTs that happened to fall across two metal strips meet all the requirements necessary for a rudimentary field-effect transistor. One metal strip is the “source” contact while the other is the “drain” contact. The silicon oxide substrate can be used as the gate oxide and adding a metal contact on the back makes the semiconducting CNT gateable.
This technique suffered from several drawbacks, which made for non-optimized transistors. The first was the metal contact, which actually had very little contact to the CNT, since the nanotube just lay on top of it and the contact area was therefore very small. Also, due to the semiconducting nature of the CNT, a Schottkey Barrier forms at the metal-semiconductor interface,[10] increasing the contact resistance. The second drawback was due to the back-gate device geometry. Its thickness made it difficult to switch the devices on and off using low voltages, and the fabrication process led to poor contact between the gate dielectric and CNT.[11]

Top-gated CNTFETs

The process for fabricating a top-gated CNTFET.
 
Eventually, researchers migrated from the back-gate approach to a more advanced top-gate fabrication process.[11] In the first step, single-walled carbon nanotubes are solution deposited onto a silicon oxide substrate. Individual nanotubes are then located via atomic force microscope or scanning electron microscope. After an individual tube is isolated, source and drain contacts are defined and patterned using high resolution electron beam lithography. A high temperature anneal step reduces the contact resistance by improving adhesion between the contacts and CNT. A thin top-gate dielectric is then deposited on top of the nanotube, either via evaporation or atomic layer deposition. Finally, the top gate contact is deposited on the gate dielectric, completing the process.
Arrays of top-gated CNTFETs can be fabricated on the same wafer, since the gate contacts are electrically isolated from each other, unlike in the back-gated case. Also, due to the thinness of the gate dielectric, a larger electric field can be generated with respect to the nanotube using a lower gate voltage. These advantages mean top-gated devices are generally preferred over back-gated CNTFETs, despite their more complex fabrication process.

Wrap-around gate CNTFETs

Sheathed CNT
Gate all-around CNT Device
Wrap-around gate CNTFETs, also known as gate-all-around CNTFETs were developed in 2008,[12] and are a further improvement upon the top-gate device geometry. In this device, instead of gating just the part of the CNT that is closer to the metal gate contact, the entire circumference of the nanotube is gated. This should ideally improve the electrical performance of the CNTFET, reducing leakage current and improving the device on/off ratio.
Device fabrication begins by first wrapping CNTs in a gate dielectric and gate contact via atomic layer deposition.[13] These wrapped nanotubes are then solution-deposited on an insulating substrate, where the wrappings are partially etched off, exposing the ends of the nanotube. The source, drain, and gate contacts are then deposited onto the CNT ends and the metallic outer gate wrapping.

Suspended CNTFETs

A suspended CNTFET device.
Yet another CNTFET device geometry involves suspending the nanotube over a trench to reduce contact with the substrate and gate oxide.[14] This technique has the advantage of reduced scattering at the CNT-substrate interface, improving device performance.[14][15][16] There are many methods used to fabricate suspended CNTFETs, ranging from growing them over trenches using catalyst particles,[14] transferring them onto a substrate and then under-etching the dielectric beneath,[16] and transfer-printing onto a trenched substrate.[15]
The main problem suffered by suspended CNTFETs is that they have very limited material options for use as a gate dielectric (generally air or vacuum), and applying a gate bias has the effect of pulling the nanotube closer to the gate, which places an upper limit on how much the nanotube can be gated. This technique will also only work for shorter nanotubes, as longer tubes will flex in the middle and droop towards the gate, possibly making touching the metal contact and shorting the device. In general, suspended CNTFETs are not practical for commercial applications, but they can be useful for studying the intrinsic properties of clean nanotubes.

CNTFET material considerations

There are general decisions one must make when considering what materials to use when fabricating a CNTFET. Semiconducting single-walled carbon nanotubes are preferred over metallic single-walled and metallic multi-walled tubes since they are able to be fully switched off, at least for low source/drain biases. A lot of work has been put into finding a suitable contact material for semiconducting CNTs; the best material to date is Pd, as its work function matches closely with that of nanotubes and it adheres to the CNTs quite well.[17]

I-V characteristics

Field effect mobility of a back-gated CNTFET device with varying channel lengths. SiO2 is used as the gate dielectric. Tool: 'CNT Mobility' at nanoHUB.org [18]
 
 
In CNT-metal contacts, the different work functions of the metal and the CNT result in the Schottky barrier at the source and drain, which are made of metals like Au, Ti, Pd and Al.[19] Even though like Schottky barrier diodes, the barriers would have made this FET to transport only one type of carrier, the carrier transport through the metal-CNT interface is dominated by quantum mechanical tunneling through the Schottky barrier. CNTFETs can easily be thinned by the gate field such that tunneling through them results in a substantial current contribution. CNTFETs are ambipolar; either electrons or holes, or both electrons and holes can be injected simultaneously.[19] This makes the thickness of the Schottky barrier a critical factor.
CNTFETs conduct electrons when a positive bias is applied to the gate and holes when a negative bias is applied, and drain current increases with increasing a magnitude of an applied gate voltage.[20] Around Vg = Vds/2, the current gets the minimum due to the same amount of the electron and hole contributions to the current.
Like other FETs, the drain current increases with an increasing drain bias unless the applied gate voltage is below the threshold voltage. For planar CNTFETs with different design parameters, the FET with a shorter channel length produces a higher saturation current, and the saturation drain current becomes also higher for the one consisting of smaller diameter keeping the length constant. For cylindrical CNTFETs, it is clear that a higher drain current is driven than that of planar CNTFETs since a CNT is surrounded by an oxide layer which is finally surrounded by a metal contact serving as the gate terminal.[21]

Theoretical derivation of drain current

Structure of a top-gate CNT transistor
Theoretical investigation on drain current of the top-gate CNT transistor has been done by T.Kazierski et al..[22] When an electric field is applied to a CNT transistor, a mobile charge is induced in the tube from the source and drain. These charges are from the density of positive velocity states filled by the source NS and that of negative velocity states filled by the drain ND,[22] and these densities are determined by the Fermi-Dirac probability distributions.
N_S = \frac{1}{2}\int_{-\infty}^{+\infty} D(E)f(E-U_{SF})\,dE
N_D = \frac{1}{2}\int_{-\infty}^{+\infty} D(E)f(E-U_{DF})\,dE
and the equilibrium electron density is
N_0 = \frac{1}{2}\int_{-\infty}^{+\infty} D(E)f(E-E_{F})\,dE .
where the density of states at the channel D(E), USF, and UDF are defined as
D(E) = D_0\frac{E}{\sqrt{E^2-(E_g/2)^2}}\Theta(E-E_g/2)
USF = EF − qVSC
UDF = EF − qVSC − qVDS.
The term, Θ(E − Eg / 2) is 1 when the value inside the bracket is positive and 0 when negative. VSC is the self-consistent voltage that illustrates that the CNT energy is affected by external terminal voltages and is implicitly related to the device terminal voltages and charges at terminal capacitances by the following nonlinear equation:
V_{SC} = \frac{-Q_t+qN_S(V_{SC})+qN_D(V_{SC})-qN_0}{C_\Sigma}
where Qt represents the charge stored in terminal capacitances, and the total terminal capacitance CΣ is the sum of the gate, drain, source, and substrate capacitances shown in the figure above. The standard approach to the solution to the self-consistent voltage equation is to use the Newton-Raphson iterative method. According to the CNT ballistic transport theory, the drain current caused by the transport of the nonequilibrium charge across the nanotube can be calculated using the Fermi–Dirac statistics.
I_{DS} = \frac{2qkT}{\pi{\hbar}}\left[ F_0 \left( \frac{U_{SF}}{kT} \right) - F_0 \left(\frac{U_{DF}}{kT}\right)\right]
Here F0 represents the Fermi–Dirac integral of order 0, k is the Boltzmann’s constant, T is the temperature, and ℏ the reduced Planck’s constant. This equation can be solved easily as long as the self-consistent voltage is known. However the calculation could be time-consuming when it needs to solve the self-consistent voltage with the iterative method, and this is the main drawback of this calculation.

Comparison to MOSFETs

CNTFETs show different characteristics compared to MOSFETs in their performances. In a planar gate structure, the p-CNTFET produces ~1500 A/m of the on-current per unit width at a gate overdrive of 0.6 V while p-MOSFET produces ~500 A/m at the same gate voltage.[23] This on-current advantage comes from the high gate capacitance and improved channel transport. Since an effective gate capacitance per unit width of CNTFET is about double that of p-MOSFET, the compatibility with high- k gate dielectrics becomes a definite advantage for CNTFETs.[21] About twice higher carrier velocity of CNTFETs than MOSFETs comes from the increased mobility and the band structure. CNTFETs, in addition, have about four times higher transconductance.

Heat dissipation

The decrease of the current and burning of the CNT can occur due to the temperature raised by several hundreds of kelvins. Generally, the self-heating effect is much less severe in a semiconducting CNTFET than in a metallic one due to different heat dissipation mechanisms. A small fraction of the heat generated in the CNTFET is dissipated through the channel. The heat is non-uniformly distributed, and the highest values appear at the source and drain sides of the channel.[24] Therefore, the temperature significantly gets lowered near the source and drain regions. For semiconducting CNT, the temperature rise has a relatively small effect on the I-V characteristics compared to silicon.

Disadvantages

Lifetime (degradation)

The carbon nanotube degrades in a few days when exposed to oxygen. There has been several works done on passivating the nanotubes with different polymers and increasing their lifetime.[25]

Reliability

Carbon nanotubes have shown reliability issues when operated under high electric field or temperature gradients. Avalanche breakdown occurs in semiconducting CNT and joule breakdown in metallic CNT. Unlike avalanche behavior in silicon, avalanche in CNTs is negligibly temperature-dependent. Applying high voltages beyond avalanche point results in Joule heating and eventual breakdown in CNTs.[26] This reliability issue has been studied, and it is noticed that the multi-channeld structure can improve the reliability of the CNTFET. The multi-channeled CNTFETs can keep a stable performance after several months, while the single-channeled CNTFETs are usually out of work after a few weeks in the ambient atmosphere.[27] The multi-channeled CNTFETs keep operating when some channels break down, this won’t happen in the single-channeled ones.

Difficulties in mass production, production cost

Although CNTs have unique properties such as stiffness, strength, and tenacity compared to other materials especially to silicon, we are still experiencing lack of technology for mass production and high production cost. To overcome the fabrication difficulties, several methods have been studied such as direct growth, solution dropping, and various transfer printing techniques.[28]

Future work

The most desirable future work involved in CNTFETs will be the transistor with higher reliability, cheap production cost, or the one with more enhanced performances. For example, such efforts could be made: adding effects external to the inner CNT transistor like the Schottky barrier between the CNT and metal contacts, multiple CNTs at a single gate,[22] channel fringe capacitances, parasitic source/drain resistance, and series resistance due to the scattering effects.


Tidak ada komentar:

Posting Komentar